Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 103 MPa | 14900 psi | ASTM D695 |
Performance Polymers IPS II PPL-A1050 PEKK (Polyetherketoneketone) Branched Standard Grade Amber pellets; neat resinInformation provided by Infinite Polymer System II. |
|||
Compressive Yield Strength | 103 MPa | 14900 psi | DIN EN ISO 604 |
Wolf Kunststoff ZEDEX® ZX-324V2T A3F PEEK, PTFE Modified Reduced friction; High wear resistance; High elasticity; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automotive Technology; Machine ToolsInformation provided by Zedex |
|||
Compressive Yield Strength | 103 MPa | 14900 psi | ASTM D695 |
Toyobo Vylopet® EMC630 PET/PBT Blend Key Feature: Flame retardant V-0 UL 94 classApplications: general and high rigidity componentsPET/PBT blends suggested for glossy surfaces. General features of Vylopet® include heat resistance, go.. |
|||
Compressive Yield Strength | 103 MPa | 14900 psi | ASTM D695 |
Adell BJ-33 Nylon 6, 15% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Compressive Yield Strength | 103 MPa | 14900 psi | ASTM D695 |
Adell BR-13 Nylon 6, 15% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Compressive Yield Strength | 103 MPa | 14900 psi | ASTM D695 |
Adell BJ-13 Nylon 6, 15% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Compressive Yield Strength | 103 MPa | 14900 psi | ASTM D695 |
Adell BR-33 Nylon 6, 15% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Compressive Yield Strength | 103 MPa | 14900 psi | ASTM D695 |
Toyobo Vylopet® EMC120K Glass Reinforced Polyester, Easy Molding Grade Flame retardant V-0 UL-94 classApplications: Electric and electronic componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and trackin.. |
|||
Compressive Yield Strength | 103 - 207 MPa | 14900 - 30000 psi | Average value: 172 MPa Grade Count:3 |
Overview of materials for PEKK, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Unreinforced". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Compressive Yield Strength | 103 MPa | 14900 psi | Average value: 103 MPa Grade Count:4 |
Overview of materials for Acrylic, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Compressive Yield Strength | 103 - 145 MPa | 14900 - 21000 psi | Average value: 127 MPa Grade Count:9 |
Overview of materials for Nylon 6, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea.. |