Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 1.48 MPa | 215 psi | Bare, typ |
Hexcel® HexWeb® CR III 3/8-5056-.0015 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Compressive Yield Strength | >= 1.48 MPa | >= 215 psi | Stabilized, min |
Hexcel® HexWeb® CR III 1/8-5052-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Compressive Yield Strength | >= 1.48 MPa | >= 215 psi | Stabilized, min |
Hexcel® HexWeb® CR III 3/16-5052-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Compressive Yield Strength | >= 1.48 MPa | >= 215 psi | Stabilized, min |
Hexcel® HexWeb® CR-PAA™ 3/16-5052-0.001 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Compressive Yield Strength | 1.48 MPa | 215 psi | Bare, typ |
Hexcel® HexWeb® CR-PAA™ 3/8-5056-0.0015 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |