Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 140 - 186 MPa | 20300 - 27000 psi | Average value: 178 MPa Grade Count:10 |
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled". Each property range of values report.. |
|||
Compressive Yield Strength | 69.0 - 186 MPa | 10000 - 27000 psi | Average value: 124 MPa Grade Count:5 |
Overview of materials for Nylon 6, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap.. |