Mechanical Properties Metric English Comments
Compressive Yield Strength 340 MPa

@Strain 10.0 %
49300 psi

@Strain 10.0 %
ASTM D695
PBI Performance Products Celazole® PBI U-60 Unfilled Polybenzimidazole Resin