Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 390 MPa @Temperature 130 °C |
56600 psi @Temperature 266 °F |
90º, Wet; EN2850 Type B |
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 52%/G1177 Glass/Carbon Fiber Information provided by HexCel |
|||
Compressive Yield Strength | 390 MPa | 56600 psi | ASTM D695 |
PBI Performance Products Celazole® PBI U-60 Unfilled Polybenzimidazole Resin U-60 grade Celazole® polybenzimidazole (PBI) resin is a organic polymer which does not burn in air and has high temperature resistance, along with excellent stability to chemicals and hydrolysis. .. |