Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.0552 - 0.0689 GPa | 8.00 - 10.0 ksi | TM R050-38 |
Resinlab® EP1295 Black Medium Viscosity, Halogen Free, Flame Retardant Epoxy Casting Resin Resinlab™ EP1295 Black is a medium viscosity, halogen free, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (.. |
|||
Compressive Modulus | 0.0552 - 168 GPa | 8.00 - 24300 ksi | Average value: 45.2 GPa Grade Count:59 |
Overview of materials for Epoxy Cure Resin This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Compressive Modulus | 0.0552 GPa | 8.00 ksi | Stabilized, typ |
Hexcel® HexWeb® HRH-10 - 1/8- 1.8 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Compressive Modulus | 0.0552 GPa | 8.00 ksi | Stabilized, typ |
Hexcel® HexWeb® HRH-10 - 3/16 - 1.8 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |