Polymer Property : Compressive Modulus = 13.8 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 13.8 GPa

@Temperature 23.9 °C
2000 ksi

@Temperature 75.0 °F
Dry; 325°F 2kpsi; ASTM D695
Park Electrochemical Nelcote® F-554 Phenolic Prepreg, Chopped Molding Compound Reinforced
Nelcote® F-554 is a high purity silica filled phenolic resin coated on Commercial or Aerospace grade silica fabric. F-554 is used in the manufacture of intermediate temperature ablative rocket nozz..
Compressive Modulus 13.8 GPa
2000 ksi
TriStar TriSteel PE Metal Backed PTFE Bearing System
Ultraflon 603 PE lined metal backed bearing system, with or without lube, high PV, high temperature... Ultraflon 603 PE Liner is a bearing grade polymer for use in lubricated or unlubricated environ..