Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 2.90 GPa | 420 ksi | ASTM D695 |
Quadrant EPP Ertalyte® PET-P, Polyester-semi-crystalline thermoplastic, extruded (ASTM Product Data Sheet) |
|||
Compressive Modulus | 2.90 GPa | 420 ksi | ASTM D695 |
Quadrant EPP Nylatron® GS Nylon, Extruded MoS2 Filled Type 66 (ASTM Product Data Sheet) |
|||
Compressive Modulus | 2.90 GPa | 420 ksi | ASTM D695 |
Quadrant EPP Quadrant Nylon 101 Extruded, Unfilled, Type 66 Natural and Black (ASTM Product Data Sheet) |
|||
Compressive Modulus | 2.90 GPa | 421 ksi | |
PBI Performance Products Celazole® TU-60 Unreinforced Melt Processable Polybenzimidazole Celazole® polybenzimidazole (PBI) resin is a unique and highly stable linear hetrocyclic polymer. PBI is characterized by high strength; excellent thermal stability, and broad chemical resistance. .. |
|||
Compressive Modulus | 2.90 GPa | 420 ksi | |
Resinlab® EP691 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP 691 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting.. |
|||
Compressive Modulus | 2.90 GPa | 420 ksi | ASTM D695 |
Quantum Nylon 6/6 Information provided by Quantum Advanced Engineering Plastics |
|||
Compressive Modulus | 2.90 GPa | 420 ksi | ASTM D695 |
Quantum Nylon 6/6 MoS2 Filled Information provided by Quantum Advanced Engineering Plastics |
|||
Compressive Modulus | 2.90 GPa | 420 ksi | ASTM D695 |
Quantum PET Information provided by Quantum Advanced Engineering Plastics |
|||
Compressive Modulus | 2.90 GPa | 421 ksi | ASTM D695 |
Saint-Gobain Meldin® 5001 Thermoplastic Bearing Material General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin.. |
|||
Compressive Modulus | 2.90 GPa | 420 ksi | |
Engineered Syntactic Systems HZ-40 Deep Water Syntactic Foam Syntactic foams are a unique combination of hollow spheres, a resin matrix, and other additives. When combined and processed properly, the constituents form a lightweight homogeneous material having.. |
|||
Compressive Modulus | 2.90 GPa | 420 ksi | TM R050-38 |
Resinlab® EP691 Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP691 is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting and ad.. |
|||
Compressive Modulus | 2.90 GPa | 420 ksi | Stabilized, typ |
Hexcel® HexWeb® CR III 1/16-5052-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |