Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 2.90 GPa | 421 ksi | |
PBI Performance Products Celazole® TU-60 Unreinforced Melt Processable Polybenzimidazole Celazole® polybenzimidazole (PBI) resin is a unique and highly stable linear hetrocyclic polymer. PBI is characterized by high strength; excellent thermal stability, and broad chemical resistance. .. |
|||
Compressive Modulus | 2.90 GPa | 421 ksi | ASTM D695 |
Saint-Gobain Meldin® 5001 Thermoplastic Bearing Material General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin.. |