Polymer Property : Secant Modulus = 2.09 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 2.09 GPa

@Strain 2.60 %,
Temperature 23.0 °C
303 ksi

@Strain 2.60 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 300PE BK602 Acetal (POM)  (Unverified Data**)
Medium-high Viscosity Acetal Homopolymer with Very Low Emissions Delrin 300PE BK602 (formerly DE20577) is a medium-high viscosity acetal homopolymer an enhanced version of Delrin 300CP with very low..
Secant Modulus 2.09 GPa

@Strain 2.12 %,
Temperature 23.0 °C
303 ksi

@Strain 2.12 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 153HSL NC010 Nylon 612  (Unverified Data**)
Unreinforced Heat Stabilized Polyamide 612 Information provided by DuPont Performance Polymers
Secant Modulus 2.09 GPa

@Strain 3.20 %,
Temperature 23.0 °C
302 ksi

@Strain 3.20 %,
Temperature 73.4 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G13L NC010 Nylon 66  (Unverified Data**)
13% Glass Reinforced Polyamide 66Zytel 70G13L NC010 is a 13% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers