Mechanical Properties Metric English Comments
Secant Modulus 2.89 GPa

@Strain 1.80 %,
Temperature 0.000 °C
420 ksi

@Strain 1.80 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 300PE BK602 Acetal (POM)  (Unverified Data**)
Medium-high Viscosity Acetal Homopolymer with Very Low Emissions Delrin 300PE BK602 (formerly DE20577) is a medium-high viscosity acetal homopolymer an enhanced version of Delrin 300CP with very low..
Secant Modulus 2.89 GPa

@Strain 1.10 %,
Temperature 23.0 °C
419 ksi

@Strain 1.10 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500TL NC010 Acetal (POM)  (Unverified Data**)
Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500TL is a medium viscosity acetal homopolymer resin containing 1.5% Teflon PTFE Micropowder. It is desi..
Secant Modulus 2.89 GPa

@Strain 1.10 %,
Temperature 23.0 °C
419 ksi

@Strain 1.10 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG500TL NC010 Acetal (POM)  (Unverified Data**)
Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact ApplicationsDelrin FG500TL medium viscosity acetal homopolymer resin containing 1.5%..
Secant Modulus 2.89 GPa

@Strain 2.80 %,
Temperature 23.0 °C
420 ksi

@Strain 2.80 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 415HP NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
15% Glass Reinforced Polyethylene Terephthalate with Excellent Impact Resistance Rynite 415HP NC010 is a 15% glass reinforced modified polyethylene terephthalate improved for easy fast processing ov..
Copyright © lookpolymers.com All Rights Reserved