Polymer Property : Puncture Energy = 60.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 60.0 J

@Temperature 23.0 °C
44.3 ft-lb

@Temperature 73.4 °F
ISO 6603-2
Covestro Makrolon® 1952 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Me..
Puncture Energy 60.0 J

@Temperature -30.0 °C
44.3 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 2256 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•..
Puncture Energy 60.0 J

@Temperature -30.0 °C
44.3 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 2258 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc..
Puncture Energy 60.0 J

@Temperature 23.0 °C
44.3 ft-lb

@Temperature 73.4 °F
ISO 6603-2
Covestro Makrolon® 2600 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Puncture Energy 60.0 J

@Temperature 23.0 °C
44.3 ft-lb

@Temperature 73.4 °F
ISO 6603-2
Covestro Makrolon® 2607 MAS167 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Puncture Energy 60.0 J

@Temperature 23.0 °C
44.3 ft-lb

@Temperature 73.4 °F
ISO 6603-2
Covestro Makrolon® 2652 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•..
Puncture Energy 60.0 J

@Temperature 23.0 °C
44.3 ft-lb

@Temperature 73.4 °F
ISO 6603-2
Covestro Makrolon® 2665 MAS071 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med..
Puncture Energy 60.0 J

@Temperature 23.0 °C
44.3 ft-lb

@Temperature 73.4 °F
ISO 6603-2
Covestro Makrolon® 2665 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medium viscosity, easy..
Puncture Energy 60.0 J

@Temperature 23.0 °C
44.3 ft-lb

@Temperature 73.4 °F
ISO 6603-2
Covestro Makrolon® 2667 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med..
Puncture Energy 60.0 J

@Temperature 23.0 °C
44.3 ft-lb

@Temperature 73.4 °F
ISO 6603-2
Covestro Makrolon® 2800 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Puncture Energy 60.0 J

@Temperature 23.0 °C
44.3 ft-lb

@Temperature 73.4 °F
ISO 6603-2
Covestro Makrolon® 2805 MAS145 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Puncture Energy 60.0 J

@Temperature 23.0 °C
44.3 ft-lb

@Temperature 73.4 °F
ISO 6603-2
Covestro Makrolon® 2805 MAS152 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Puncture Energy 60.0 J

@Temperature 23.0 °C
44.3 ft-lb

@Temperature 73.4 °F
ISO 6603-2
Covestro Makrolon® 3100 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig..
Puncture Energy 60.0 J

@Temperature 23.0 °C
44.3 ft-lb

@Temperature 73.4 °F
ISO 6603-2
Covestro Makrolon® 3107 MAS167 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig..
Puncture Energy 60.0 J

@Temperature 23.0 °C
44.3 ft-lb

@Temperature 73.4 °F
ISO 6603-2
Covestro Makrolon® 3152 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•..
Puncture Energy 60.0 J

@Temperature 23.0 °C
44.3 ft-lb

@Temperature 73.4 °F
ISO 6603-2
Covestro Makrolon® 3158 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc..
Puncture Energy 60.0 J

@Temperature 23.0 °C
44.3 ft-lb

@Temperature 73.4 °F
ISO 6603-2
Covestro Makrolon® ET3117 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc..
Puncture Energy 60.0 J

@Temperature 23.0 °C
44.3 ft-lb

@Temperature 73.4 °F
ISO 6603-2
Covestro Makrolon® FU1007 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Furniture applications..
Puncture Energy 60.0 J

@Temperature 23.0 °C
44.3 ft-lb

@Temperature 73.4 °F
ISO 6603-2
Covestro Makrolon® FU4007 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Furniture applications..
Puncture Energy 60.0 J

@Temperature 23.0 °C
44.3 ft-lb

@Temperature 73.4 °F
ISO 6603-2
Covestro Makrolon® ET2613 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• Medium vi..
Puncture Energy 60.0 J

@Temperature 23.0 °C
44.3 ft-lb

@Temperature 73.4 °F
ISO 6603-2
Covestro Makrolon® ET3127 Polycarbonate
Makrolon® polycarbonate resinMain characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characterist..
Puncture Energy 60.0 J

@Temperature 23.0 °C
44.3 ft-lb

@Temperature 73.4 °F
ISO 6603-2
Covestro Makrolon® ET3227 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc..
Puncture Energy 60.0 J

@Temperature 23.0 °C
44.3 ft-lb

@Temperature 73.4 °F
ISO 6603-2
Covestro Makrolon® LED2643 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• LED lighting, optics, ..
Puncture Energy 60.0 J

@Temperature 23.0 °C
44.3 ft-lb

@Temperature 73.4 °F
ISO 6603-2
Covestro Makrolon® LQ2647 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Optical lens, safety g..