Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Heat Seal Strength, Ultimate | 12.9 N | 2.90 lb (f) | at 150°C, 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method |
Dow TUFLIN™ HS-7041 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Good Strength High Output Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a (with Restrictions) TUFLIN™ HS-7041 NT 7 is a half melt, ethylene-hexene copolymer, designe.. |
|||
Heat Seal Strength, Ultimate | 12.9 N | 2.90 lb (f) | at 160°C, 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method |
Dow TUFLIN™ HS-7066 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7066 NT 7 is a fractional melt, ethylene-hexene copolymer, designed for good toughness and stiffness. Th.. |