Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Stiffness | 965 MPa | 140000 psi | Olsen Stiffness; ASTM D747 |
Mitsui TPX® RT18 Methylpentene Copolymer, Transparent Grade TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |
|||
Flexural Stiffness | 965 MPa | 140000 psi | Olsen Stiffness; ASTM D747 |
Mitsui TPX® RT18 XB Methylpentene Copolymer TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |