Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 205 MPa | 29700 psi | ISO 2039-1 |
Nilit FRIANYL A63 KV50 Nylon 6.6 for injection molding, 50% glass ball reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 205 MPa | 29700 psi | ISO 2039-1 |
Quadrant EPP Techtron® PPS unfilled, extruded (ISO Data) This unfilled polyphenylene sulfide based material is ideal for structural applications in corrosive environments or as a PEEK replacement at less demanding temperatures. Very good dimensional stabi.. |
|||
Ball Indentation Hardness | 205 MPa | 29700 psi | ISO 2039-1 |
Lanxess Durethan® BM 240 000000 Nylon 6, Mineral Reinforced PA 6, injection molding, 40% mineral, isotopic properties, low warpageInformation provided by LANXESS. |
|||
Ball Indentation Hardness | 205 MPa | 29700 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® BGM-30 X PA6-(GF+MD)30 Product description: Grilon BGM-30 X is a heat stabilized PA 6 injection molding grade with a 30 % reinforcement combination (mineral and glass fiber). Grilon BGM-30 X has the following important pr.. |
|||
Ball Indentation Hardness | 205 MPa | 29700 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® TSG-30/4 H black 9836 PA666-GF30 Information provided by EMS Grivory |
|||
Ball Indentation Hardness | 205 MPa | 29700 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® TSG-30/4 H black 9839 PA666-GF30 Information provided by EMS Grivory |
|||
Ball Indentation Hardness | 205 MPa | 29700 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TSGL-50/4 black 9833 PA666-GF50 Product description: Grilon TSGL-50/4 black is based on a heat stabilized semicrystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 black is characterized by the following key-p.. |
|||
Ball Indentation Hardness | 205 MPa @Load 98.0 kg, Time 30.0 sec |
29700 psi @Load 216 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultrason® E 2010 G4 MR SW 15102 20% Glass Filled PESU Information provided by BASF |
|||
Ball Indentation Hardness | 205 MPa @Load 36.5 kg |
29700 psi @Load 80.5 lb |
dry; ISO 2039-1 |
Azoty Tarnow™ Tarnamid® T-27 GF30 Polyamide 6 - Glass Fiber Reinforced 30% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Ball Indentation Hardness | 205 MPa @Load 36.5 kg |
29700 psi @Load 80.5 lb |
ISO 2039-1 |
Azoty Tarnow™ Tarnamid® T-27 MW30 Polyamide 6 - Mineral Reinforced 30% Mineral filled, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High mechani.. |
|||
Ball Indentation Hardness | 205 MPa | 29700 psi | ISO 2039-1 |
BASF Ultrason E 2010 G4 20% Glass Filled PES Ultrason E 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength. |