Mechanical Properties Metric English Comments
Ball Indentation Hardness 375 MPa
54400 psi
ISO 2039-1
Quadrant EPP Duratron® PBI CU60 compression moulded (ISO Data)
Duratron CU60 PBI is very “clean” in terms of ionic impurity and does not outgas (except water). These characteristics make this material extremely attractive to high-tech industries such as semic..
Ball Indentation Hardness 375 MPa
54400 psi
H 961/30; ISO 2039/P1
Hexion UP 802 Unsaturated Polyester Resin, High Surface Quality, Low Shrinkage, High Arc Resistance
Polyester molding compound, inorganically filled, glass fiber reinforced, styrene free, high dimensional stability, very slight post shrinkage, good mechanical properties, increased electrical value..