Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 39.0 MPa | 5660 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® 2D 25 W 20 HL X black 9992 PA612-I Product Description: Grilamid 2D 25 W 20 HL X black 9992 is a semi-flexible high viscosity, plasticized, high impact and highly heat resistant polyamide 612 (PA612) grade. Unique properties of Gril.. |
|||
Ball Indentation Hardness | 39.0 MPa | 5660 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® 2D 25 W 20 X black PA612-I Product Description: Grilamid 2D 25 W 20 X black 9992 is a semi-flexible high viscosity, plasticized, high impact, heat and UV resistant extrusion grade based on polyamide 612 (PA612). Unique proper.. |
|||
Ball Indentation Hardness | 39.0 MPa | 5660 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® 2D 25 W 20 X nat PA612-I Product Description: Grilamid 2D 25 W 20 X natural 9992 is a semi-flexible high viscosity, plasticized, high impact, heat and UV resistant extrusion grade based on polyamide 612 (PA612). Unique pro.. |
|||
Ball Indentation Hardness | 39.0 MPa | 5660 psi | ISO 2039-1 |
Azoty Tarnow™ TARFLEN SM-S15G2 PTFE Tarflen SM1 reinforced with 15% glass fibers and 2% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |