Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 924 MPa @Temperature 71.0 °C |
134000 psi @Temperature 160 °F |
|
Hexcel® HexPly® F155 Epoxy Resin, T3T095 Carbon Tape Hexcel designation: TXX095-12"-F155; Various fibersInformation provided by HexCel |
|||
Compressive Yield Strength | 924 MPa @Temperature 25.0 °C |
134000 psi @Temperature 77.0 °F |
0°, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, A280-5H Fiber Information provided by HexCel |