Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 407 MPa @Temperature 163 °C |
59000 psi @Temperature 325 °F |
0° |
Hexcel® HexPly® 954-2A Curing Cyanate Resin, Quartz Fiber Reinforced 8 Harness Satin Fabric Information provided by HexCel |