Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 469 MPa @Temperature 24.0 °C |
68000 psi @Temperature 75.2 °F |
|
Hexcel® F161 Epoxy Resin, 7781 Glass Fabric Hexcel designation: 7781-38"-F161; Fiber: 75-1/0Information provided by HexCel |
|||
Compressive Yield Strength | 469 MPa @Temperature 232 °C |
68000 psi @Temperature 450 °F |
Phase II (Prepreg stored in freezer 4 months at -9°C and exposed to 60 days at RT) |
Hexcel® HexPly® F650 Bismaleimide Resin with Graphite F3T584 fabric reinforcement Aging Data, (T300-3K, 8 H.S.); Laminate Physicals: 59.6% Fiber volume, 34.0% Resin content, 1.0% VoidsInformation provided by HexCel |
|||
Compressive Yield Strength | 469 MPa @Temperature 93.0 °C |
68000 psi @Temperature 199 °F |
Dry |