Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 410 MPa @Temperature 71.0 °C |
59500 psi @Temperature 160 °F |
Wet |
Hexcel® HexPly® F593 Epoxy Resin, W3G282 Carbon Fabric Hexcel designation: W3G282-42"-F593; Fiber: Amoco T-300/3kInformation provided by HexCel |