Mechanical Properties Metric English Comments
Compressive Yield Strength 924 MPa

@Temperature 71.0 °C
134000 psi

@Temperature 160 °F
Hexcel® HexPly® F155 Epoxy Resin, T3T095 Carbon Tape
Hexcel designation: TXX095-12"-F155; Various fibersInformation provided by HexCel
Compressive Yield Strength 924 MPa

@Temperature 25.0 °C
134000 psi

@Temperature 77.0 °F
0°, Dry
Hexcel® HexPly® 8552 Epoxy Matrix, A280-5H Fiber
Information provided by HexCel