Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.350 J/cm² @Temperature -30.0 °C |
1.67 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Nilit Nilamid A H2 FR HF2 Unfilled, Flame Retardant PA66/6 Co-Polymer Description: Nilamid A H2 FR HF2 is an unfilled, flame retardant NYLON 66/6 co-polymer that does not contain halogen or red phosphorous. This product combines excellent flow characteristics and extr.. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature -30.0 °C |
1.67 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Nilit Nilamon B3 H7 GK 35 15% Glass Fiber, 25% Mineral Reinforced PA6 Description: Nilamon B3 H7 GK 35 provides a combination between low warpage and high stiffness, while retaining a good impact strength. It has a high heat aging resistance, so that it is suitable fo.. |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179-1/1eA |
Quadrant EPP Ketron® 1000 PEEK unfilled, extruded (ISO Data) Ketron PEEK-1000 stock shapes are produced from virgin polyetheretherketone resin and offer the highest toughness and impact strength of all Ketron PEEK grades. Both Ketron PEEK-1000 natural & black.. |
|||
Charpy Impact, Notched | 0.350 - 0.450 J/cm² @Temperature 23.0 °C |
1.67 - 2.14 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eA |
Raschig Group 5562 DAP Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona.. |
|||
Charpy Impact, Notched | 0.350 - 1.10 J/cm² | 1.67 - 5.24 ft-lb/in² | Average value: 0.636 J/cm² Grade Count:12 |
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are.. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYplex PMMA 700 Acrylic Glass Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYshine PBT D201 GF20 PBT, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.350 - 0.800 J/cm² @Temperature -30.0 - -30.0 °C |
1.67 - 3.81 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.525 J/cm² Grade Count:4 |
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar.. |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® C 52G1 V25 Grey R7035 (XC 1329/A) PA6, DRY Description: Polyamide 6, Glass-filled, glow-wire modified, color stabilized, lubricated for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Application.. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis HG385MO Polypropylene HG385MO is a polypropylene homopolymer intended for injection molding. This grade combines unique Borstar® reactor design with Borstar® nucleation technology to produce highly-crystalline polyprop.. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis HG430MO Polypropylene HG430MO is a polypropylene homopolymer intended for injection molding. This polymer product is characterized by a superior impact resistance. This grade has ductile failure in falling weight impact .. |
|||
Charpy Impact, Notched | 0.350 - 0.550 J/cm² | 1.67 - 2.62 ft-lb/in² | ISO 179 |
Vyncolit G885 Novolac Phenolic Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties. Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179 |
Total PPH 10042 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 10042 is a nucleated antistatic homopolymer. PPH 10042 is characterized by high fluidity for high speed injection of thin wall articles such as dairy pots and tubs, salad .. |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Crastin® SO653 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 20% Glass Bead Filled Polybutylene Terephthalate with Low Warpage CharacteristicsCrastin SO653 NC010 is a 20% glass bead filled polybutylene terephthalate resin for injection molding. It has isotrop.. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature -30.0 °C |
1.67 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DuPont Performance Polymers Crastin® SO653 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 20% Glass Bead Filled Polybutylene Terephthalate with Low Warpage CharacteristicsCrastin SO653 NC010 is a 20% glass bead filled polybutylene terephthalate resin for injection molding. It has isotrop.. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature -40.0 °C |
1.67 ft-lb/in² @Temperature -40.0 °F |
ISO R179 |
Arkema Group ORGASOL® 3502 D Nat 1 Copolyamide 6/12 Information provided by Arkema Group |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | dry; ISO 179 1eA |
Azoty Tarnow™ Tarnamid® T-27 GF10 MX10 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grade, reinforced with 10% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning, good surface quality.T.. |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | 1eA; ISO 179 |
Azoty Tarnow™ TARNOFORM 300 TF4 POM Tribological modified grade with addition of 20% PTFE, with very low coefficient of friction and wear.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | Conditioned; ISO 179/IeA |
Addiplast Addilene H 290 M20F Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179 |
BASF Ultramid® 8202C HS PA6 (Dry) Ultramid 8202C HS is a heat stabilized, low viscosity, PA6 injection molding homopolymer possessing a modified crystalline structure for increased property performance and faster cycles. It is also.. |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179 |
BASF Ultramid® 8202C PA6 (Dry) Ultramid 8202C is a modified crystalline and low viscosity, nylon 6 injection molding homopolymer. It is also available in heat stabilized (Ultamid 8202C HS) and/or pigmented versions. Its unique .. |
|||
Charpy Impact, Notched | >= 0.350 J/cm² @Temperature 23.0 °C |
>= 1.67 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
AKG Polymers Vision PP PPH Jazz0502dark Polypropylene Homopolymer Compound Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin.. |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179-1 |
Vyncolit W5020 Glass Filled Novolac Phenolic Novolac resin based, glass fiber and glass bead reinforced. High dimensional stability and excellent chemical resistance at high temperatures in hydraulic brake fluids. Used in the ABS system.Inform.. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis HF136MO Polypropylene HF136MO is a polypropylene homopolymer intended for injection molding. This grade is characterized by a good combination of mechanical and flow properties. This polymer is a CR (controlled rheology.. |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179/1eA |
BASF Ultradur B 4300 G2 High Speed Unc. 10% Glass Filled PBT Ultradur B 4300 G2 High Speed Unc. is a high flow, fast cycling with low warpage, 10% glass filled, pigmented black, injection molding PBT for industrial parts, rigid tough and dimensional stable ap.. |
|||
Charpy Impact, Notched | 0.350 J/cm² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
IRPC Polimaxx Polene 3375RM Polypropylene Random Copolymer CHARACTERISTICS: GOOD EXTRUDABILITY, GOOD ADHESIVE, HIGH SPEED APPLICATIONS: EXTRUSION COATING FOR COATED WOVEN BAGS AND TARPAULINS |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179/1eA |
Lucite International Elvakon® 4451 Super Low Gloss Acrylic Capstock Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable prot.. |
|||
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | Conditioned; ISO 179/IeA |
Addiplast Addilene PMD 50203 Flame Retardant Polypropylene Flame retardant, unreinforced, with halogensInformation provided by Addiplast. |