Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL A63 CV-CM 0515 9005/Z Powder-coatable nylon 6.6 for injection molding, 15% ceramic filled Powder-coatable nylon 6.6 for injection molding, with conductive carbon blackInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 KV50 Nylon 6.6 for injection molding, 50% glass ball reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | ISO Data |
Americas Styrenics Styron® 666D Polystyrene
(discontinued **) STYRON® 666D general purpose polystyrene resin is used in injection molding applications, particularly for medical, pharmaceutical and food uses. It offers excellent clarity, intermediate flow char.. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | ISO Data, Low Temp |
Americas Styrenics Styron® XL-8023VC High Impact Polystyrene
(discontinued **) STYRON® XL-8023 VC high impact polystyrene is designed to provide molders of VCR cassettes with the impact and gloss they require, at economics and processability highly advantaged over ABS resins... |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 KF30 M2 Nylon 6.6 for injection molding, 30% short glass fiber reinforced and 2% molybdenum disulphide lubricated Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 KV30 Nylon 6.6 for injection molding, 30% glass ball reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -40.0 °C |
1.90 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL B63 W-GV15 Nylon 6 for injection molding, 15% glass fiber reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature 23.0 °C |
1.90 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Victrex® ST™ STG45 PolyEtherKetoneEtherKetoneKetone, Unreinforced Product Description:High performance thermoplastic material, unreinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, depth filtered granules for injection moulding, standard flow, .. |
|||
Charpy Impact, Notched | 0.400 J/cm² - NB | 1.90 ft-lb/in² - NB | Average value: 1.85 J/cm² Grade Count:25 |
Overview of materials for Nylon 12, Extrusion/Tubing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Extrusion/Tubing Grade". Each property range of values reported is minimum and maximum values .. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | |
LATI Latimass 82-02 D030 PA12 Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics ULTEM 3452 PEI (Europe-Africa-Middle East) 45% Glass fiber and mineral filled, enhanced flow Polyetherimide (Tg 217C) with enhanced dimensional stability. Resin is RoHS compliant. UL94 V0 and 5VA listing in recognized colors. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature 23.0 °C |
1.90 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Ultem HATX200 PEI+PCE (Asia Pacific) High flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compli.. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics ULTEM HU1000E PEI Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (.. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Valox® 4012 PBT (Europe-Africa-Middle East) VALOX 4012 is a 10% high strength glass fibre reinforced PBT injection moulding resin with improved mechanical properties. Applications: connectors. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Valox® DR48 - CS1049 PBT (Europe-Africa-Middle East) VALOX DR48 is a 15 % glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot.. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Valox® DR48V PBT (Europe-Africa-Middle East) VALOX DR48V is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot.. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | ISO 179 |
Teijin Panlite® G-3330M Isotropic, Glass Fiber Reinforced Polycarbonate Resin Reinforced with 30 % of special GF and least anisotropy grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need good appearance and mechanical propertyPrecisio.. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -40.0 °C |
1.90 ft-lb/in² @Temperature -40.0 °F |
ISO 179-1/1eA |
Styron INSPIREâ„¢ TF0808S(U) Polypropylene TF0808S(U) is a talc filled PP exhibiting high impact resistance and a high stiffness. It is particularly well suited for low wall thickness bumper skins. INSPIRE TF0808S for painted parts INSPIRE .. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
ISO 179/2C |
SABIC Innovative Plastics Valox® 4512 PBT+PC (Europe-Africa-Middle East) 10% GF FR PBT/PC Blend |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® X6320 PBT+PC (Asia Pacific) X6320 is a mineral filled PBT/PC resin developed for automotive painted doorhandles. Key advantages are excellent surface finish, easy processing and paint quality. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature 23.0 °C |
1.90 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Noryl GTX APS8740 PPE+PPS (Asia Pacific) Noryl* APS8740 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can be e.. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | ISO 179-1 |
Unitika M1030DH PA6, Dry Nano composite nylonInformation provided by Unitika Ltd. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature 30.0 °C |
1.90 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® BG-30 FR PA6-GF30 FR Information provided by EMS Grivory |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature 30.0 °C |
1.90 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® GM-4H PA*-MD40 Product description: Grivory GM-4H natural is a 40 % mineral reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyamide. G.. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® E51HSB NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized High Viscosity Polyamide 66 Zytel E51HSB NC010 is a high molecular weight heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by .. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature 30.0 °C |
1.90 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® BR 40 PA6 Product description: Grilon BR 40 is a medium viscosity, unreinforced, heat stabilized PA6 grade for injection mounding and extrusion applications. Grilon BR 40 has the following important propertie.. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® 157HSL BK010 Nylon 612
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 612 Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |