Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.300 - 0.400 J/cm²
1.43 - 1.90 ft-lb/in²
Injection; ISO 179/1eA
Raschig Group 6502 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler
Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi..
Charpy Impact, Notched 0.250 - 0.400 J/cm²

@Temperature 23.0 °C
1.19 - 1.90 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eA
Raschig Group 6552 DAIP
Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi..
Charpy Impact, Notched 0.200 - 0.400 J/cm²
0.952 - 1.90 ft-lb/in²
Injection; ISO 179/1eA
Raschig Group DECAL® 1760 Phenolic
Glass-fiber reinforced phenolic molding compound. Very good electrical properties, good chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals an..
Charpy Impact, Notched 0.200 - 0.400 J/cm²
0.952 - 1.90 ft-lb/in²
Injection; ISO 179/1eA
Raschig Group DECAL® 2061 Phenolic
Wood flour reinforced phenolic molding compound. Good electrical properties, chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals and PCAs and ..
Charpy Impact, Notched 0.200 - 0.400 J/cm²
0.952 - 1.90 ft-lb/in²
Injection; ISO 179/1eA
Raschig Group DECAL® 5431 Phenolic
Organically and inorganically filled phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/..
Charpy Impact, Notched 0.200 - 0.400 J/cm²
0.952 - 1.90 ft-lb/in²
Compression; ISO 179/1eA
Raschig Group DECAL® 572R Phenolic
Glass-fiber reinforced phenolic molding compound. Exceptional heat resistance with regard to maintaining surface finish and mechanical properties, outstanding mechanical properties, excellent rotati..
Charpy Impact, Notched 0.200 - 0.400 J/cm²
0.952 - 1.90 ft-lb/in²
Compression; ISO 179/1eA
Raschig Group DECAL® 666/8 Phenolic
Glass-fiber reinforced phenolic molding compound with mineral fillers. High heat resistance, reduced mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This prod..
Charpy Impact, Notched 0.200 - 0.400 J/cm²
0.952 - 1.90 ft-lb/in²
Injection and Compression; ISO 179/1eA
Raschig Group DECAL® 666/8/2B Phenolic
Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meets the allowe..
Charpy Impact, Notched 0.200 - 0.400 J/cm²

@Temperature 23.0 °C
0.952 - 1.90 ft-lb/in²

@Temperature 73.4 °F
Injection and Compression; ISO 179/ 1eA
Raschig Group EPOXIDUR® 3580 EP Epoxy
Glass-fiber reinforced and mineral filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties even with thin wall thicknesses and high temperatures. This prod..
Charpy Impact, Notched 0.200 - 0.400 J/cm²
0.952 - 1.90 ft-lb/in²
Injection and Compression; ISO 179/1eA
Raschig Group EPOXIDUR® 3581 S ZC EP Epoxy Molding Compound
Inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very good sealing connection on ..
Charpy Impact, Notched 0.200 - 0.400 J/cm²
0.952 - 1.90 ft-lb/in²
Injection and Compression; ISO 179/1eA
Raschig Group EPOXIDUR® 3581 T-1 EP Epoxy, Molded, Glass Fiber Filler
Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very ..
Charpy Impact, Notched 0.250 - 0.400 J/cm²
1.19 - 1.90 ft-lb/in²
Injection; ISO 179/1eA
Raschig Group MELOPAS® 156 MF Melamine
Glass fiber reinforced Melamine molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 200..
Charpy Impact, Notched 0.300 - 0.400 J/cm²
1.43 - 1.90 ft-lb/in²
Injection; ISO 179/1eA
Raschig Group RALUPOL® 4802 UP Polyester
Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u..
Charpy Impact, Notched 0.300 - 0.400 J/cm²
1.43 - 1.90 ft-lb/in²
Injection; ISO 179/1eA
Raschig Group RALUPOL® 802 UP Polyester
Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength, good heat resistance. This product meets the allowed up..
Charpy Impact, Notched 0.300 - 0.400 J/cm²
1.43 - 1.90 ft-lb/in²
Injection; ISO 179/1eA
Raschig Group RALUPOL® 804 UP Polyester
Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy m..
Charpy Impact, Notched 0.200 - 0.400 J/cm²

@Temperature 23.0 °C
0.952 - 1.90 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eA
Raschig Group RALUPOL® 8601 UP
Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic moulding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical stren..
Charpy Impact, Notched 0.200 - 0.400 J/cm²

@Temperature 23.0 °C
0.952 - 1.90 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eA
Raschig Group RALUPOL® 8602 UP
Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic molding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical streng..
Charpy Impact, Notched 0.199 - 0.400 J/cm²
0.947 - 1.90 ft-lb/in²
Average value: 0.271 J/cm² Grade Count:7
Overview of materials for Phenolic, Novolac, Flock Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Flock Filled". Each property range of values reported is minimum and maximum values o..
Charpy Impact, Notched 0.200 - 0.400 J/cm²
0.952 - 1.90 ft-lb/in²
ISO 179
Vyncolit X658 Novolac Phenolic
Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties and a very good dimensional stability.USES: Complex precision parts.Information provided by ..
Charpy Impact, Notched 0.250 - 0.400 J/cm²
1.19 - 1.90 ft-lb/in²
ISO 179
Vyncolit X681 Novolac Phenolic
Glass fiber filled phenolic molding compound with excellent mechanical properties and a low coefficient of friction. Tribological compound with PTFE additive.USES: Water pump seals and self-lubrica..
Charpy Impact, Notched 0.300 - 0.400 J/cm²

@Temperature -30.0 - -30.0 °C
1.43 - 1.90 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.350 J/cm² Grade Count:2
Overview of materials for Nylon 6, Nucleated
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Nucleated". Each property range of values reported is minimum and maximum values of appropriate..
Charpy Impact, Notched 0.250 - 0.400 J/cm²
1.19 - 1.90 ft-lb/in²
ISO 179
Vyncolit X682 Novolac Phenolic
Glass fiber, glass bead and graphite filled phenolic molding compound with excellent mechanical properties and a low coefficient of friction.USES: Water pump seals and self-lubricating bearings.Info..
Charpy Impact, Notched 0.200 - 0.400 J/cm²
0.952 - 1.90 ft-lb/in²
Compression; ISO 179/1eA
Raschig Group DECAL® 152CL Phenolic
Glass-fiber and mineral reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meet..
Charpy Impact, Notched 0.400 - 0.400 J/cm²

@Temperature -20.0 - -20.0 °C
1.90 - 1.90 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 0.400 J/cm² Grade Count:1
Overview of materials for Polypropylene with 10% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be..
Copyright © lookpolymers.com All Rights Reserved