Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.410 - 1.40 J/cm² | 1.95 - 6.66 ft-lb/in² | Average value: 0.675 J/cm² Grade Count:4 |
Overview of materials for Nylon 12, Graphite Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Graphite Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Charpy Impact, Notched | 0.410 J/cm² | 1.95 ft-lb/in² | ISO 179 |
BASF Capron® 8224 HSL Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Charpy Impact, Notched | 0.410 J/cm² @Temperature -30.0 °C |
1.95 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS Lustran® 488 Key Features:UnfilledSuitable processing methods:Injection molding |
|||
Charpy Impact, Notched | 0.410 J/cm² | 1.95 ft-lb/in² | ISO 179/1eA |
Polyplastics Duranex® 7400W Polybutylene Terephthalate (PBT), Super low warpage, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Charpy Impact, Notched | 0.410 J/cm² @Temperature -30.0 °C |
1.95 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® AMN P20 TLD Nylon 12, Flexible, Injection Grade (Conditioned) Designation ISO 1874-PA12-P,MHLR,14-005Flexible grade for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Good impact strength. Flexibility and .. |
|||
Charpy Impact, Notched | 0.410 J/cm² @Temperature -30.0 °C |
1.95 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® MA 4411 Nylon 12, Flexible Tubing Grade (Dry) Designation ISO 1874-PA12-HI,EHL,22-003Flexible grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized.Flexibility. High burst pressure and impact strength. Fit fo.. |
|||
Charpy Impact, Notched | 0.410 J/cm² | 1.95 ft-lb/in² | ISO 179 |
BASF Ultramid® B3GM35 Q643 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid B3GM35 Q643 is a 40% combined glass-fiber and mineral reinforced injection molding PA6 grade. |
|||
Charpy Impact, Notched | 0.410 J/cm² | 1.95 ft-lb/in² | |
Arkema Group Rilsan® AMN G8 TLD Nylon 12, Graphite Filled (Dry) Designation ISO 1874-PA12,MHLS,14-010,CD05Rigid grade with graphite filler for injection molding. Available colors: steel gray. Light and heat stabilized. Mold-release agent.Low friction coefficient.. |