Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | ISO 179-1/1eA |
Quadrant EPP Ertalon® 6 SA PA 6, extruded (ISO Data) This material offers an optimal combination of mechanical strength, stiffness, toughness, mechanical damping properties and wear resistance. These properties, together with good electrical insulatin.. |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature -30.0 °C |
2.62 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Nilit FRIANYL A63 V2 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, flame retardant, free of halogen and phosphorus.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | |
LATI Larton GK/400 PPS, Glass/Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers / Carbon fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa &.. |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature -30.0 °C |
2.62 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Borealis Daplen™ KSR4525 Polypropylene Reactor Elastomer Modified Daplen KSR4525 is a reactor elastomer modified polypropylene intended for injection molding. Daplean KSR4525 is a material with excellent impact/stiffness ratio. The grade is available in natural .. |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis RJ470MO Polypropylene, Transparent Random Copolymer RJ470MO is a specially modified highly-transparent polypropylene random copolymer with very high melt flow rate and is designed for high-speed injection molding and contains nucleating and demolding.. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | ISO 179 |
Total PPC 9642 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 9642 is nucleated heterophasic copolymer. PPC 9642 is characterized by improved stiffness, creep resistance, high impact resistance, excellent antistatic properties and has been f.. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | IS0179 |
Zhejiang Juner 302-G10 10% Glass Fibre Reinforced, Flammable Resistant, and Low Separate Out Mode Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | IS0179-1:2000 |
Zhejiang Juner JEPPB006 High Glossy PP Applications: Electric Rice CookerInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Sorona® 3015GV NC010 Polytrimethylene Terephthalate (PTT) 15% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3015GV NC010 is a 15% glass reinforced PTT resin containing 31% renewably sourced ingredients by weight (37% based on pol.. |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature -30.0 °C |
2.62 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Pebax® 7033 SN 01 Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE (PEBA) hardness 70 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: Sport (Football shoe sole, ski top lay.. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | ISO 179-1eA |
Barlog Plastics KEBAFORM C 274 VT POM Copolymer unreinforced, antistatic POMInformation provided by BARLOG plastics GmbH. |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature -30.0 °C |
2.62 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
BASF Ultraform N 2320 003 UNC Q600 POM Ultraform N 2320 003 UNC Q600 is a rapidly solidifying grade of POM for injection molding. Contains a mold release agent. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | ISO 179 |
BASF Ultraform N 2320 U03 UNC Q600 POM Ultraform N2320 U03 UNC Q600 is a rapidly freezing UV stabilized general-purpose injection molding grade. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | ISO 179 |
BASF Ultramid® 1403-2 BK ND3007 PA66 (Dry) |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | ISO 179/1eA |
BASF Ultrason S 2010 PSU Ultrason S 2010 is an unreinforced, medium viscosity standard injection molding PSU grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req.. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | Conditioned; ISO 179/IeA |
Addiplast Addilene J 290 M20F Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Sorona® 3015G NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& 15% Glass Reinforced Polytrimethylene Terephthalate with Resin Made from Bio-PDO Sorona 3015G NC010 is a 15% glass reinforced PTT resin containing 31% renewably sourced ingredients by weight (37% ba.. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® 101F BKB009 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101F BKB009 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont.. |