Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact, Notched = 0.810 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.810 J/cm²
3.85 ft-lb/in²
ISO 179/1eA
Solvay TECHNYLSTARâ„¢ S 216L2 V30 PA6, 30% glass filled, DRY
Description: TECHNYLSTAR polyamide reinforced with 30% GF, UV stabilized, for Injection molding. Available in: Europe and North AmericaProduct Applications: TECHNYLSTAR TM S 216L2 V30 BLACK is chara..
Charpy Impact, Notched 0.810 J/cm²
3.85 ft-lb/in²
ISO 179/1eA
Polyplastics Duranex® CN7130 Polybutylene Terephthalate (PBT), Low friction, Low wear, GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Charpy Impact, Notched 0.810 J/cm²
3.85 ft-lb/in²
ISO 179/1eA
Polyplastics Duranex® HN7330 Polybutylene Terephthalate (PBT), Low warpage, 30% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Charpy Impact, Notched 0.810 J/cm²
3.85 ft-lb/in²
ISO 179/1eA
Polyplastics Duranex® 3306 Polybutylene Terephthalate (PBT), Higher gloss, Better surface appearance, 30% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Charpy Impact, Notched 0.810 J/cm²

@Temperature -30.0 °C
3.85 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® AZM 23 T6LD Nylon 12, 23% Glass Fiber Filled (Conditioned)
Designation ISO 1874-PA12,MHLR,16-050,GF23Rigid grade with glass fiber filler (23%) for injection molding. Available colors: black and natural. Reinforced light and heat stabilizing agent. Mold-rele..
Charpy Impact, Notched 0.810 J/cm²
3.85 ft-lb/in²
ISO 179/1eA
Cathay PA514 Renewable Engineering Polyamide
Cathay engineering polyamides contain 26-100% renewably sourced material. Advantages: Operates at similar conditions to PA66; Suitable for injection, compounding and extrusion; Stable mechanical pr..
Copyright © lookpolymers.com All Rights Reserved