Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.299 J/cm² | 1.42 ft-lb/in² | ASTM D256 |
Plenco 6015 Phenolic, Briquette, Injection Molded PLENCO 06015 is a glass and mineral filled phenolic molding compound offering improved mechanical strength, dimensional stability and excellent electrical properties. 06015 is available in black.Inf.. |