Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 2.20 J/cm² @Temperature -30.0 °C |
10.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Nilit Nilamid B3 H ZC Unfilled, Low Temperature Impact Resistant PA6 Description: Nilamid B3 H ZC has outstanding impact performance, even at minus temperatures. It is widely used for components subjected to high shock loads. Applications include bicycle components, .. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Asia Pacific) Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.4mm and 5VB at 1... |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics EXTEM UH1016 TPI Blend (Europe-Africa-Middle East) High heat amorphous TPI Blend, Chemical Resistant, High Flow |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179/1eA |
Pasargad Polymer Peyvand Pasamid 3P-H2130B1 Nylon 66, 30% Glass Fiber Reinforced Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | |
Ineos ABS Lustran® 348 Key Features:UnfilledSuitable processing methods:Injection molding |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO Data |
Styron Magnum™ 9095 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO Data |
Styron Magnumâ„¢ FG960 ABS, High Impact MAGNUM ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS .. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO Data, Low Temp |
Styron Pulse® 1350 ABS + Polycarbonate PULSE® 1350 Engineering resin offers a superior total performance with a balance of heat resistance, practical toughness, high and low temperature impact strength retention and ease of processing.. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO Data, Low Temp |
Styron Pulse® 930 ABS + Polycarbonate PULSE® 930 Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at room temperature. PULSE 930 Engineering resin has been used i.. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity.. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA (Europe-Africa-Middle East) NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity.. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics XYLEX HX7409HP PC+POLYESTER Low flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change (MoC), biocompatible (ISO 10993 or USP Class VI).. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics LNP VERTON RX10409D PA 66 LNP* VERTON* RX10409D is a compound based on Nylon 66 containing proprietary fillers. Added feature of this grade is: Structural. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179 |
Polyram Polytron P50B07 Polypropylene, 50% Long Glass Fiber, UV Stabilized A chemically coupled 50% long glass fiber reinforced black polypropylene, heat stabilized, UV stabilized for injection molding applications.Information provided by Polyram. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179 |
Polyram Polytron P40N11 Polypropylene, 40% Long Glass Fibers A chemically coupled 40% long glass fiber reinforced natural polypropylene, heat stabilized, for injection molding applications.Information provided by Polyram. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® 1SVX-65H nat PA1010-GF65 Product Description: Grilamid 1SVX-65H natural is a 65% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile: Raw materials based on renewable resources E.. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® 1SVX-65H nat PA1010-GF65 Product Description: Grilamid 1SVX-65H natural is a 65% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile: Raw materials based on renewable resources E.. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6600 GV 30 HWCP 30% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179-2 |
Denka MALECCA K-090 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® TR 90 NZ PAMACM12-I Product description: Grilamid TR grades are transparent thermoplastic polyamides based on aliphatic and cycloaliphatic blocks. Grilamid TR 90 NZ offers a variety of interesting properties such as: o.. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179 |
Chi Mei Polylac® PA-746H ABS - High Flow Super high flow, medium impact |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature -20.0 °C |
10.5 ft-lb/in² @Temperature -4.00 °F |
After conditioning at 23°C/50%RH; ISO 179/Af |
Arkema Group Orgalloy® LE 60 ES Polyamide Alloy Polyamide Alloy, Blow Molding of Technical PartsInformation provided by Arkema Group |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature -30.0 °C |
10.5 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Orgalloy® LT 4060 Flexible Nylon Alloy (Conditioned) Very flexible polyamide alloy: easy to process, low moisture absorption, good mechanical properties at low temperature. Demonstrates a good balance of properties eg, high flexibility (200 MPa), good.. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179 |
BASF Ultramid® TG7S BK-102 35% Glass Filled PA6 (Dry) Ultramid TG7S is a 34% glass reinforced, heat stabilized, impact modified nylon 6 injection molding grade. It was developed to meet the demanding requirements of the first North American seat cushi.. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | After conditioning at 23°C/50%RH; ISO 179/Af |
Arkema Group Orgalloy® RS 6030 Polyamide 6 Alloy 30% Glass Fiber reinforced Polyamide Alloy, Rigid grade, Nylon 6 basedMolding of Engineering PartsInformation provided by Arkema Group |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179/1eA |
BASF Ultramid® A3EG6 30% Glass Filled PA66 (Conditioned) Ultramid A3EG6 is a 30% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
Charpy Impact, Notched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179 |
Chi Mei Polylac® PA-763A ABS - Flame Retardant F.R. High Heat |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DuPont Performance Polymers Sorona® MT3401 NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® MT3401 NC010 is a medium toughened polytrimethylene terephthalate resin containing 29% renewably sourced ingredients by weight. It was initially coded SE38001.Information provided by DuPont.. |