Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | >= 2.50 J/cm² | >= 11.9 ft-lb/in² | ISO 179 |
Murtfeldt Muralen® Black Antistatic Polyethylene, Conductive Muralen® is based on high molecular weight polyethylene (PE-HMW) and is ideally suited for use in applications that require the generally impressive material properties of polyethylene. Because of.. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | ISO 179 |
PolyOne OnForce™ LFT PP-50LGF/001 Natural Polypropylene Homopolymer (PP Homopolymer) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® FXC630ME PC+ABS (Asia Pacific) PC+ABS, ECO-conforming flame retardant with metallic or pearlescent appearance. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Lexan® 920 PC (Europe-Africa-Middle East) LEXAN 920 is a low viscosity flame retardant grade, especially suitable for electrical applications. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent .. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer (Asia Pacific) Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent .. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer (Europe-Africa-Middle East) 6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer (Asia Pacific) Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele.. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | |
Eastman Eastar DN101 PCTG Copolyester
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
Charpy Impact, Notched | 2.50 J/cm² - NB | 11.9 ft-lb/in² - NB | Average value: 11.7 J/cm² Grade Count:57 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | ISO 179 1eA |
Lehmann & Voss LUVOCOM® 50/GF/10/TF/18/SI/2/GY5 Polycarbonate, with glass fiber, PTFE, lubricant modified Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | ISO 179 1eA |
Lehmann & Voss LUVOCOM® 50/TF/15/BK Polycarbonate, with PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL PX6120 PPE+PS Noryl PX6120 is an unfilled material with good flow, high Impact and chemical resistance against cleaners. Noryl PX6120 is developed for personal care appplications. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Styron CALIBREâ„¢ MEGARAD 2081-HD-15 2 Polycarbonate Resin Overview: CALIBREâ„¢ MEGARAD 2081 HD-15 2 polycarbonate resin provides end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed .. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | ISO 179/1eA |
Borealis Borsoft™ SF203CF Soft Polypropylene Copolymer for Extrusion Coating Borsoft SF203CF is a new statistic-heterophasic propylene-ethylene copolymer suitable for coating applications. Its polymer structure permits perfect adhesion to certain products. According to the.. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature 30.0 °C |
11.9 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® ELX 40 HNZ TPA Product description: Grilon ELX 40 H NZ is a high viscosity, heat stabilized, impact modified, thermoplastic PA6 elastomer for extrusion blow moulding applications. Grilon ELX 40 H NZ has the follow.. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® TSGZ-30 PA666-GF30 Product description: Grilon TSGZ-30 is a heat stabilized, normal viscosity, and impact modified PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSGZ-30 has the following important p.. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature 30.0 °C |
11.9 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 5106 (GVL-4H V0) PA*-GF40 Product description: Grivory XE 5106 black 9915 is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide. The product is flame retarded and reinf.. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature 30.0 °C |
11.9 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® XE 5106 (GVL-4H V0) PA*-GF40 Product description: Grivory XE 5106 black 9915 is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide. The product is flame retarded and reinf.. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® BG-50 H PA6-GF50 Product description: Grilon BG-50 H is a high heat stabilized PA6 injection molding grade with 50% glass fibers. Grilon BG-50 H has the following important properties: High stiffnessHigh heat resist.. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Conditioned) Description: 50% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness as well as for electric insulating parts.Information provided by BASF |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | Conditioned; ISO 179/IeA |
Addiplast Addinyl PMD 20164 Nylon 6 High resistance to repeated impactsInformation provided by Addiplast. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
|
BASF Luranyl® KR 2460/3 Polyphenylene Ether + Styrene-Butadiene Blend Flame retardant grade with very high heat resistance; used for precision parts and where the material must withstand high injection temperatures (e.g. heater-fan impellers).Data was collected by ISO.. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | ISO 179 |
Orbilan ORBILAN® PE 500 HMW-PE Orbilan PE 500 plastic is used as cutting boards for the food industry and gastronomy, in refrigeration chambers as ram protection and for swing doors as well as at sports grounds for sheets or hand.. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Conditioned) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultramid® B3WG5 BK 00564 25% Glass Filled PA6 (Conditioned) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |