Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.400 - 0.450 J/cm²
1.90 - 2.14 ft-lb/in²
Injection; ISO 179/1eA
Raschig Group 2557 AMC Polyester
Glass fiber reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, exceptional processability with short cycle time and low ..
Charpy Impact, Notched 0.350 - 0.450 J/cm²

@Temperature 23.0 °C
1.67 - 2.14 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eA
Raschig Group 5562 DAP
Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona..
Charpy Impact, Notched 0.350 - 0.450 J/cm²

@Temperature 23.0 °C
1.67 - 2.14 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eA
Raschig Group 5563 DAP
Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona..
Charpy Impact, Notched 0.250 - 0.450 J/cm²
1.19 - 2.14 ft-lb/in²
Compression; ISO 179/1eA
Raschig Group 6551 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler
Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi..
Charpy Impact, Notched 0.150 - 0.450 J/cm²
0.714 - 2.14 ft-lb/in²
Average value: 0.211 J/cm² Grade Count:32
Overview of materials for Phenolic, Novolac, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral Filled". Each property range of values reported is minimum and maximum values..
Charpy Impact, Notched 0.281 - 0.450 J/cm²
1.34 - 2.14 ft-lb/in²
Average value: 0.357 J/cm² Grade Count:3
Overview of materials for Phenolic/Rubber; Molded
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic/Rubber; Molded". Each property range of values reported is minimum and maximum values of approp..
Charpy Impact, Notched 0.350 - 0.450 J/cm²
1.67 - 2.14 ft-lb/in²
ISO 179
Vyncolit 4451 XB Novolac Phenolic
Organic and mineral filled phenolic molding compound with excellent mechanical properties (highest notched impact strength).USES: Fuse holders, brush holders, circuit breakers, automotive ignition a..