Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.400 - 2.50 J/cm²
1.90 - 11.9 ft-lb/in²
ISO.179 DN.53453
Polimersan Plastics POLIPA® (PA 6) Polyamide
POLIPA® PA6 (POLYAMIDE) is produced by poly condensation of e-aminoacid and by the help of d-carbon acid and d-amine poly condensation. Its characteristics depend upon the numbers of the main struc..
Charpy Impact, Notched 0.250 - 2.50 J/cm²

@Temperature -30.0 - -20.0 °C
1.19 - 11.9 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.841 J/cm² Grade Count:49
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim..
Charpy Impact, Notched 0.500 - 2.50 J/cm²

@Temperature -30.0 - -30.0 °C
2.38 - 11.9 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.08 J/cm² Grade Count:13
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Extrusion Grade". Each property range of values reported is minimum an..
Charpy Impact, Notched 0.900 - 2.50 J/cm²

@Temperature -40.0 - -20.0 °C
4.28 - 11.9 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 1.52 J/cm² Grade Count:14
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m..
Charpy Impact, Notched 0.400 - 2.50 J/cm²
1.90 - 11.9 ft-lb/in²
ISO.179 DN.53453
Polimersan Plastics POLIPA® (PA 6) Polyamide
POLIPA® PA6 (POLYAMIDE) is produced by poly condensation of e-aminoacid and by the help of d-carbon acid and d-amine poly condensation. Its characteristics depend upon the numbers of the main struc..
Charpy Impact, Notched 0.100 - 2.50 J/cm²
0.476 - 11.9 ft-lb/in²
Average value: 0.992 J/cm² Grade Count:68
Overview of materials for Polystyrene, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a..
Charpy Impact, Notched 0.500 - 2.50 J/cm²

@Temperature -30.0 - -20.0 °C
2.38 - 11.9 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 1.49 J/cm² Grade Count:13
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and ..
Charpy Impact, Notched 0.200 - 2.50 J/cm²

@Temperature -30.0 - 30.0 °C
0.952 - 11.9 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 0.832 J/cm² Grade Count:29
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl..
Charpy Impact, Notched 0.650 - 2.50 J/cm²
3.09 - 11.9 ft-lb/in²
Average value: 1.62 J/cm² Grade Count:20
Overview of materials for Nylon 12, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. ..
Charpy Impact, Notched 1.20 - 2.50 J/cm²
5.71 - 11.9 ft-lb/in²
Average value: 1.84 J/cm² Grade Count:21
Overview of materials for Nylon 12, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. ..
Charpy Impact, Notched 0.800 - 2.50 J/cm²
3.81 - 11.9 ft-lb/in²
Average value: 1.40 J/cm² Grade Count:6
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo..
Charpy Impact, Notched 0.700 - 2.50 J/cm²
3.33 - 11.9 ft-lb/in²
Average value: 1.62 J/cm² Grade Count:5
Overview of materials for Polycarbonate, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app..
Charpy Impact, Notched 0.800 - 2.50 J/cm²
3.81 - 11.9 ft-lb/in²
Average value: 1.72 J/cm² Grade Count:6
Overview of materials for Polycarbonate, Glass + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value..