Polymer Property : Charpy Impact, Notched = 2.80 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 2.80 J/cm²
13.3 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Cycolac® MG38 ABS (Europe-Africa-Middle East)
Very high impact ABS. Toughness/rigidity. Good fatigue resistance.
Charpy Impact, Notched 2.80 J/cm²

@Temperature 23.0 °C
13.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Polykemi AB POLYabs R00 ABS, High Impact
Information provided by Polykemi AB
Charpy Impact, Notched 2.80 J/cm²

@Temperature 23.0 °C
13.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Polykemi AB POLYabs R00 UV4 ABS, High Impact, UV Stabilized
Information provided by Polykemi AB
Charpy Impact, Notched 2.80 J/cm²

@Temperature 23.0 °C
13.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Polykemi AB POLYelast TPE R44 Thermoplastic Elastomer
Information provided by Polykemi AB
Charpy Impact, Notched 2.80 J/cm²

@Temperature 23.0 °C
13.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Polykemi AB POLYfill PPC T1010 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
Charpy Impact, Notched 2.80 J/cm²
13.3 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Cycoloy® CY6414 PC (Asia Pacific)
Charpy Impact, Notched 2.80 J/cm²
13.3 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Cycoloy® CY6414 PC (Europe-Africa-Middle East)
Flame retardant modified PC blend using non-brominated and non-chlorinated flame retardant systems, offering high heat for application in appliances, lighting and electrical market.
Charpy Impact, Notched 2.80 J/cm²

@Temperature 23.0 °C
13.3 ft-lb/in²

@Temperature 73.4 °F
Radici Radilon® S RV350 (cond.) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Charpy Impact, Notched 2.80 J/cm²

@Temperature 23.0 °C
13.3 ft-lb/in²

@Temperature 73.4 °F
Injection Molded; ISO 179
PolyOne Bergamid™ B70 G30 BK Polyamide 6 (Nylon 6)
Information provided by PolyOne
Charpy Impact, Notched 2.80 J/cm²

@Temperature -30.0 °C
13.3 ft-lb/in²

@Temperature -22.0 °F
80*10*4mm, Cut; ISO 179/1eA
SABIC Innovative Plastics SABIC STAMAX 40YM240 PP
SABIC® STAMAX 40YM240 is a 40% long glass fiber reinforced polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMDS is 16497161...
Charpy Impact, Notched 2.80 J/cm²

@Temperature 23.0 °C
13.3 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66
High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Americas region.
Charpy Impact, Notched 2.80 J/cm²

@Temperature 23.0 °C
13.3 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66 (Asia Pacific)
High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Asia Pacific region.
Charpy Impact, Notched 2.80 J/cm²
13.3 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics NORYL ENV131 PPE+HIPS (Europe-Africa-Middle East)
Noryl* ENV131 is an unfilled modified polyphenylene ether resin developed for extrusion process. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V1 rating ..
Charpy Impact, Notched 2.80 J/cm²
13.3 ft-lb/in²
ISO 179/1eA
Borealis Daplen™ KSR4525 Polypropylene Reactor Elastomer Modified
Daplen KSR4525 is a reactor elastomer modified polypropylene intended for injection molding. Daplean KSR4525 is a material with excellent impact/stiffness ratio. The grade is available in natural ..
Charpy Impact, Notched 2.80 J/cm²

@Temperature 23.0 °C
13.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179
CP-Polymer-Technik Wellamid® 6000/42 Nylon 6, Polymer Modified, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Charpy Impact, Notched 2.80 J/cm²
13.3 ft-lb/in²
conditioned; ISO 179/1eA
EMS-Grivory Grivory® LCL-3 H anthracite PA12-CF30
Product description: Grilamid LCL-3H anthracite is based on a heat stabilized PA12 and 30% long carbon fibers. Grilamid LCL-3H anthracite is characterized by the following key-properties: high stiff..
Charpy Impact, Notched 2.80 J/cm²
13.3 ft-lb/in²
After conditioning at 23°C/50%RH; ISO 179/Af
Arkema Group Orgalloy® LE 60 HM Polyamide Alloy
Polyamide Alloy, Film and PackagingInformation provided by Arkema Group
Charpy Impact, Notched 2.80 J/cm²
13.3 ft-lb/in²
1eA; ISO 179
Azoty Tarnow™ TARNOFORM 200 HI4 POM
Rubber modified grade with very high impact strength and damping capacity.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Charpy Impact, Notched 2.80 J/cm²

@Temperature 23.0 °C
13.3 ft-lb/in²

@Temperature 73.4 °F
Radici Radilon® A RV500 (cond.) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Charpy Impact, Notched 2.80 J/cm²

@Temperature -30.0 °C
13.3 ft-lb/in²

@Temperature -22.0 °F
80*10*4mm, Cut; ISO 179/1eA
SABIC Innovative Plastics SABIC STAMAX 40YM243 PP
SABIC® STAMAX 40YM243 is a 40% long glass fiber reinforced UV stabilized polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMDS ..
Charpy Impact, Notched 2.80 J/cm²
13.3 ft-lb/in²
ISO 179
Polyram Polytron A50B01 Nylon 6.6, 50% Long Fiber Glass
50% Long fiber glass reinforced black Nylon 6.6, heat stabilized for injection molding applications.Information provided by Polyram.