Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.810 J/cm² | 3.85 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYLSTARâ„¢ S 216L2 V30 PA6, 30% glass filled, DRY Description: TECHNYLSTAR polyamide reinforced with 30% GF, UV stabilized, for Injection molding. Available in: Europe and North AmericaProduct Applications: TECHNYLSTAR TM S 216L2 V30 BLACK is chara.. |
|||
Charpy Impact, Notched | 0.810 J/cm² | 3.85 ft-lb/in² | ISO 179/1eA |
Polyplastics Duranex® CN7130 Polybutylene Terephthalate (PBT), Low friction, Low wear, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Charpy Impact, Notched | 0.810 J/cm² | 3.85 ft-lb/in² | ISO 179/1eA |
Polyplastics Duranex® HN7330 Polybutylene Terephthalate (PBT), Low warpage, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Charpy Impact, Notched | 0.810 J/cm² | 3.85 ft-lb/in² | ISO 179/1eA |
Polyplastics Duranex® 3306 Polybutylene Terephthalate (PBT), Higher gloss, Better surface appearance, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Charpy Impact, Notched | 0.810 J/cm² @Temperature -30.0 °C |
3.85 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® AZM 23 T6LD Nylon 12, 23% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-050,GF23Rigid grade with glass fiber filler (23%) for injection molding. Available colors: black and natural. Reinforced light and heat stabilizing agent. Mold-rele.. |
|||
Charpy Impact, Notched | 0.810 J/cm² | 3.85 ft-lb/in² | ISO 179/1eA |
Cathay PA514 Renewable Engineering Polyamide Cathay engineering polyamides contain 26-100% renewably sourced material. Advantages: Operates at similar conditions to PA66; Suitable for injection, compounding and extrusion; Stable mechanical pr.. |