Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.880 J/cm² | 4.19 ft-lb/in² | ISO 179/1eA |
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi.. |
|||
Charpy Impact, Notched | 0.880 J/cm² | 4.19 ft-lb/in² | |
LATI Latamid 66 H2 G/35-V0HF1 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Eur.. |
|||
Charpy Impact, Notched | 0.880 J/cm² | 4.19 ft-lb/in² | Type 1, Edgewise; ISO 179 |
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA), 25% Glass Fiber (Dry) Amodel® AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s.. |
|||
Charpy Impact, Notched | 0.880 J/cm² | 4.19 ft-lb/in² | ISO 179/1eA |
Polyplastics Duranex® 7407 Polybutylene Terephthalate (PBT), Super low warpage, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Charpy Impact, Notched | 0.880 J/cm² | 4.19 ft-lb/in² | ISO 179/1eA |
Polyplastics Duranex® CRN7030 Polybutylene Terephthalate (PBT), Low gas generation, Low contact contamination, FR, UL approved regrind 50%, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Charpy Impact, Notched | 0.880 J/cm² | 4.19 ft-lb/in² | |
Arkema Group Rilsan® AMN P20 TLD Nylon 12, Flexible, Injection Grade (Dry) Designation ISO 1874-PA12-P,MHLR,14-005Flexible grade for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Good impact strength. Flexibility and .. |
|||
Charpy Impact, Notched | 0.880 J/cm² @Temperature -30.0 °C |
4.19 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
BASF Ultraform N 2200 G53 UNC Q600 25% Glass Filled POM Ultraform N2200 G53 UNC Q600 is a 25% glass fiber reinforced POM injection molding grade with enhanced stiffness and toughness. |