Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXM1413T PC Copolymer PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® ML7682 PC Copolymer (Asia Pacific) Lexan ML7682 resin is a flame retardant polycarbonate blend featuring high flow, good processability, good impact, good heat resistance, and UV stability. It is of non-chlorine and non-bromine flame.. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | ISO Data |
Americas Styrenics Styron® 489M High Impact Polystyrene
(discontinued **) STYRON® 489M high impact polystyrene resin is a high flow resin with excellent impact. When used unmodified for the manufacture of food contact articles STYRON 489M complies with the US Food, Drug .. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature -40.0 °C |
7.61 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL B63 HS-GV30 Nylon 6 for injection molding, 30% glass fiber reinforced Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® XHT1141 PC (Asia Pacific) XHT1141 is a high flow, high heat polycarbonate copolymer. It is the lowest heat product in the LEXAN* XHT portfolio. It is available in a range of opaque and limited transparent colors. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® XHT1141 PC (Europe-Africa-Middle East) XHT1141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | DIN 53453 |
IRPC Polimaxx Polene GG3245 High Density Polyethylene CHARACTERISTICS: EXCELLENT ENVIRONMENTAL STRESS CRACKING RESISTANCE (ESCR) EXCELLENT IMPACT STRENGTH, GOOD PROCESSABILITY, HIGH TOUGHNESSAPPLICATIONS: BLOW MOLDING/ SHEET/ THERMOFORMING EXTRUSION CO.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
80x10x4mm, r=0.25; V-notch; ISO 179/1eA |
SYNTHOS Forsan® 449 Acrylonitrile Butadiene Styrene (ABS) High flow, high gloss, suitable for electroplating.Applications: General purpose, intricate and thin-walled productsHousehold appliances, vacuum cleaners, heels, toys, fan grilles, etc.Synthos was f.. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | ISO 179/1EA-1993 |
Solvay Technyl® A 246M Nylon 66, Impact Grade, EH0 Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Technyl A 246m offers an excellent notched impact resistance at low temperatures makin.. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® B 218 Black 21 N PA66/6, Conditioned Description: Unreinforced copolyamide PA 66/6 , heat stabilized , medium viscosity, for injection molding.Available in: EuropeProduct Applications: TECHNYL® B 218 offers all of the primary proper.. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® C 216 V15 PA6, 15% glass filled, Eh 50 Description: TECHNYL C 216 V15 is a polyamide 6 with 15% of glass fiber.Colors: it is marketed in the black color and natural.Available in: Asia Pacific and EuropeMain Properties: Dimensional stabil.. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | ISO Data |
Styron Magnum™ 348 ABS, Low Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | ISO Data |
Styron Magnum™ SPD 214 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL PVX516 PPE PREVEX* PVX516 resin is a high flow, non FR grade, 110 C HDT |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics ULTEM AUT210 PEI (Asia Pacific) Transparent Polyetherimide (Tg 227 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature o.. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | ISO 179-1 |
Unitika B2040G50 PA66, 50% Glass Fiber Reinforced, Dry Information provided by Unitika Ltd. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 MRGV 25/15 HWCP 25% Mineral and 15% Glass Fiber Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® GCL-3H anthracite PA*-CF30 Product description: Grivory GCL-3H anthracite is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide. The product is reinforced by 30% long ca.. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | ISO 179-2 |
Denka MALECCA K-300 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | 50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® 70G30HSL NC010 Nylon 66
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G30HSL NC010 is a 30% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perform.. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® 70G43HSLA BK099 Nylon 66
(Unverified Data**) 43% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G43HSLA BK099 is a 43% glass fiber reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont .. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | After conditioning at 23°C/50%RH; ISO 179/Af |
Arkema Group Orgalloy® RS 6620 Polyamide 6.6 Alloy 20% Glass Fiber reinforced Polyamide Alloy, Rigid grade, Nylon 6.6 basedMolding of Engineering PartsInformation provided by Arkema Group |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | |
Arkema Group Rilsan® MA 4420 Nylon 12, Flexible Tubing Grade (Dry) Designation ISO 1874-PA12-HI,EHL,22-003Flexible grade for tubes extrusion. Available color: black. Light and heat stabilized.Flexibility. High burst pressure and impact strength. Fit for use in a wi.. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | ISO 179 |
BASF Ultramid® NBX-0025 NF2001 PA66 (Conditioned) Ultramid NBX-0025 NF2001 is a specialty, unfilled PA6/6. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Akro-Plastic Akroloy® PA GF 60 (2844) PA 6.6 & PA6I/6T Conditioned, 60% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 30.0 °C |
7.61 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 4208 black 9992 PA612-I Product description: Grilamid XE 4208 black 9992 is a semiflexible high viscosity, plasticized, high impact and highly heat resistant polyamide 612 (PA612) extrusion grade. Unique properties of Gril.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 0.000 °C |
7.61 ft-lb/in² @Temperature 32.0 °F |
ISO 179/1eA |
Borealis Borstar® HE3490-LS Black High Density Polyethylene for Pressure Pipes Borstar HE3490-LS is a black, bimodal, high density polyethylene classified as an MRS 10.0 material (PE100) produced by the advanced Borstar technology. Well dispersed carbon black gives outstanding.. |