Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.188 J/cm | 0.352 ft-lb/in | ASTM D256 |
Plenco 2408 Phenolic, Granular, Compression Molded PLENCO 02408 is a general purpose, organic filled phenolic molding compound, offering excellent cosmetic characteristics and improved electrical strength properties. UL recognized under component fi.. |
|||
Izod Impact, Notched | 0.188 J/cm | 0.352 ft-lb/in | ASTM D256 |
Plenco 3557 Phenolic, Granular, Transfer Molded PLENCO 03557 is a woodflour and mineral filled phenolic molding compound offering excellent dielectric strength values at elevated temperatures while maintaining mechanical strength properties. UL r.. |