Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.240 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.450 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Maxxam™ STFPP.1220 BK-L Polypropylene, Unspecified (PP, Unspecified) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Izod Impact, Notched | >= 0.240 J/cm @Temperature 23.0 °C |
>= 0.450 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
NIZHNEKAMSKNEFTEKHIM PE 2062U (62111) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | |
Reliance Industries Polypropylene - Virgin Polypropylene Information provided by Reliance Industries |
|||
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 LNP* Konduit* PX08321 a compound based on PA6 resins containing mineral. Added features include: Thermally Conductive. |
|||
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | ASTM D256 |
Omni Plastics OmniTech™ HPP TF20 V0 Flame Retardant OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and .. |
|||
Izod Impact, Notched | 0.240 J/cm @Temperature -30.0 °C |
0.450 ft-lb/in @Temperature -22.0 °F |
ASTM D256A |
Total Finaclear® 530 Clear Impact Polystyrene
(discontinued **) Finaclear® 530 is a clear high styrenic styrene-butadiene (SBS) elastomer, providing dramatically improved impact properties and tear resistance to finished articles, when used in blends with other.. |
|||
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | |
Reliance Industries Polypropylene - Talc filled Information provided by Reliance Industries |
|||
Izod Impact, Notched | 0.240 - 7.74 J/cm | 0.450 - 14.5 ft-lb/in | Average value: 0.842 J/cm Grade Count:66 |
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |
|||
Izod Impact, Notched | 0.240 - 0.290 J/cm | 0.450 - 0.543 ft-lb/in | Average value: 0.259 J/cm Grade Count:15 |
Overview of materials for Phenolic, Novolac, Impact Grade, Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Impact Grade, Filled". Each property range of values reported is minimum and maximum .. |
|||
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | ASTM D256 |
Plenco 7466 Phenolic, Granular, Transfer Molded
(discontinued **) Two-Stage Phenolic. PLENCO 07466 is a flock cotton and mineral filled phenolic molding compound offering excellent heat resistance and dimensional stability. UL recognized under component file E406.. |
|||
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP ML004LS PP LNP* LUBRICOMP* ML004LS is a compound based on Polypropylene resin containing 20% PTFE. Added features of this matLNP* Lubricomp* ML004LS is a compound based on Polypropylene resin containing PTFE... |
|||
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | ASTM D256 |
Sumitomo Bakelite North America E 8354-19189-2 Electrical Encapsulation Grade Epoxy Glass and mineral reinforced epoxy molding compound, formulated for the encapsulation of devices requiring high quality and thermal shock resistance.Information provided by Vyncolit, a Sumitomo Bak .. |
|||
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | ASTM D256 |
Sumitomo Bakelite Durez® 22257 Phenolic, Injection Grade Durez 22257 Black Phenolic is a two-stage, asbestos-free, medium impact molding material. It is designed for appliance and electrical applications where additional mechanical strength is required. .. |
|||
Izod Impact, Notched | 0.240 J/cm @Temperature 22.8 °C |
0.450 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Teknor Apex Sinpolene CPP1050 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Calcium Carbonate Filler, 40% Filler by Weight Features: Homopolymer Uses: Appliance Components; Furniture; Housings F.. |
|||
Izod Impact, Notched | >= 0.240 J/cm | >= 0.450 ft-lb/in | ASTM D256, Notch |
Cresset Powers Cress-Alon™ A2600 2.6 r.v. Compounding Grade Nylon 6, Dry As Molded Neat resin, for compounding.Information provided by Cresset Powers Ltd. |
|||
Izod Impact, Notched | >= 0.240 J/cm | >= 0.450 ft-lb/in | ASTM D256, Notch |
Cresset Powers Cress-Alon™ A2700 2.7 r.v. Compounding Grade Nylon 6, Dry As Molded Neat resin, for compounding.Information provided by Cresset Powers Ltd. |
|||
Izod Impact, Notched | 0.240 - 0.260 J/cm | 0.450 - 0.487 ft-lb/in | ASTM D256A |
DSM Somos® WaterClear® Ultra 10122 Optically Clear, Colorless, Rigid, Stereolithography Resin DescriptionDSM Somos® WaterClear Ultra 10122 is a next generation optically clear resin with ABS like properties and good temperature resistance. It produces colorless, functional, accurate parts .. |
|||
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | ASTM D256 |
Bapolene® 4071 Polypropylene, Fiber/Injection Grade Bapolene PP4071 is a high flow PP homopolymer for staple and continuous filament applications as well as general purpose injection molding. This resin exhibits good melt and thermal stability.Appli.. |
|||
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | ASTM D256 |
Aclo Accucomp Polystyrene GS0500L Low Impact |
|||
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | ASTM-D256 |
Braskem PH 0950 HOMO Polypropylene Homopolymer PH 0950 is a medium melt flow rate homopolymer with an antiblocking agent. PH 0950 is specially designed for twisted films produced by cast or blown film extrusion. It exhibits excellent optical pro.. |
|||
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | ASTM D256 |
Asahi Kasei Thermofil P-40TC-0158 40% Talc Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Izod Impact, Notched | 0.240 J/cm @Temperature -40.0 °C |
0.450 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Ashley Polymers Ashlene® L925 Nylon 12 A flexible Nylon 12 with exceptional toughness, excellent abrasion and chemical resistance, outstanding low temperature performance, dimensional stability and low moisture absorption. The natural c.. |
|||
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | ASTM D256-06 |
Proto3000 Objet VeroWhite FullCure830 Rapid Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | ASTM D256A |
Sumitomo Bakelite North America FM 4004 Fiberglass and Mineral Reinforced Phenolic Novolac FM 4004 is a fiberglass and mineral reinforced phenolic novolac compound. This compound exhibits excellent dimensional stability and good strength at elevated temperatures, and conforms to the requ.. |
|||
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | ASTM D256A |
Sumitomo Bakelite North America RX® 1-501AN Mineral Filled Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ.. |
|||
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | ASTM D256 |
Sumitomo Bakelite North America RX® 1-501N Mineral Filled Diallyl Phthalate Mineral filled diallyl ortho-phthalate molding compound which meets the requirements of ASTM D5948 Type MDG.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | ASTM D256A |
Sumitomo Bakelite North America RX® 1-510N Mineral Filled Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ.. |
|||
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | ASTM D256 |
Plaslok 7021 Black Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 7021 is the replacement material for .. |