Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.260 J/cm @Temperature 23.0 °C |
0.487 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Reliance Industries Repol H100EY Polypropylene REPOL Polypropylene H100EY is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Izod Impact, Notched | 0.260 - 1.81526 J/cm @Temperature -50.0 - -17.8 °C |
0.487 - 3.40073 ft-lb/in @Temperature -58.0 - 0.000 °F |
Average value: 0.562 J/cm Grade Count:19 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Izod Impact, Notched | 0.260 - 1.30 J/cm @Temperature -30.0 - -30.0 °C |
0.487 - 2.44 ft-lb/in @Temperature -22.0 - -22.0 °F |
Average value: 0.758 J/cm Grade Count:6 |
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and .. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256A |
Total Finaclear® 520 Clear Impact Polystyrene
(discontinued **) Finaclear® 520 is a clear high styrenic styrene-butadiene (SBS) elastomer, providing dramatically improved impact properties and tear resistance to finished articles. Complemented by inherent repr.. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256A |
Total Finaclear® 521 Clear Impact Polystyrene
(discontinued **) Finaclear® 521 is a clear high styrenic styrene-butadiene (SBS) elastomer, providing dramatically improved impact properties and tear resistance to finished articles, when used in blends with othe.. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP KONDUIT PX11422 PA 6 LNP* KONDUIT* is a compound based on Nylon 6 resin containing thermally conductive fillers. Added feature of this material is Electrically Conductive. |
|||
Izod Impact, Notched | 0.260 J/cm @Temperature 23.0 °C |
0.487 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl TN240 PPE+PS PPE+PS blend. Unfilled. Transparent. Good flow. Scratch resistant. Injection molding. Suitable for housewares, personal care and small appliance applications.This data was supplied by SABIC-IP for t.. |
|||
Izod Impact, Notched | 0.260 J/cm @Temperature 23.0 °C |
0.487 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl TN240 PPE+PS (Asia Pacific) PPE+PS. Transparent. High flow, scratch resistant. Injection molding. Housewares and small appliances applications.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP ML004S PP (Asia Pacific) LNP* Lubricomp* ML004S is a compound based on Polypropylene resin containing PTFE. Added features of this material include: Internally Lubricated, Heat Stabilized. |
|||
Izod Impact, Notched | 0.260 J/cm @Temperature 23.0 °C |
0.487 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp RFM62 PA 66 (Asia Pacific) LNP* Lubricomp* RFM62 is a compound based on Nylon 66 resin containing Glass Fiber, Mineral.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RN001S PA 66 LNP* LUBRICOMP* RN001S is a compound based on Nylon 66 resin containing 2% MOS2. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RN001S PA 66 (Asia Pacific) LNP* Lubricomp* RN001S is a compound based on Nylon 66 resin containing MOS2. Added features of this material include: Internally Lubricated, Heat Stabilized. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP UAL22S PPA LNP* LUBRICOMP* UAL22S is a compound based on Polyphthalamide resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM DU319 PEI Transparent Polyetherimide blend. ECO Conforming. US FDA and EU Food Contact Compliant in recognized colors. |
|||
Izod Impact, Notched | 0.260 J/cm @Temperature -30.0 °C |
0.487 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 7062HP PBT ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP AH0230A ABS (Europe-Africa-Middle East) LNP THERMOCOMP* AH0230A is a compound based on Acrylonitrile Butadiene Styrene resin. Added features of this material include: High Specific Gravity. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP AX08306 ABS (Asia Pacific) LNP* Thermocomp* AX08306 is a compound based on Acrylonitrile Butadiene Styrene resin containing Mineral. |
|||
Izod Impact, Notched | 0.260 J/cm @Temperature 23.0 °C |
0.487 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp WFB51 PBT LNP THERMOCOMP* WFB51 is a compound based on Polybutylene Terephalate resin containing Glass Bead, Glass Fiber. Added features of this material include: Low Warpage.This data was supplied by SABIC-.. |
|||
Izod Impact, Notched | 0.260 J/cm @Temperature 23.0 °C |
0.487 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl PKN4766 PPE+PS (Asia Pacific) PPE+PS. Translucent. FDA compliant. High flow. Extrusion. Microwavable. Food packaging uses.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.260 J/cm @Temperature -30.0 °C |
0.487 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 7062HP PBT (Asia Pacific) ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP MB008S PP LNP* THERMOCOMP* MB008S is a compound based on Polypropylene resin containing 40% Glass Bead. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256A |
Sumitomo Bakelite North America FM 4005X4648 Fiberglass Reinforced Phenolic Novolac FM 4005X4648 a fiberglass reinforced phenolic novolac molding compound formulated to increase thermal conductivity and electrical conductance. This material also exhibits low post mold shrinkage.In.. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256 |
A. Schulman PP 1248-01 Polypropylene High-Flow Homopolymer Polypropylene DescriptionPolypropylene PP 1248-01 is a high-flow homopolymer polypropylene nucleated and anti static designed for the high speed molding of thin-walled, multi-cavity parts. ApplicationTypical appl.. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256 |
A. Schulman PP 1248-01 Polypropylene High-Flow Homopolymer Polypropylene DescriptionPolypropylene PP 1248-01 is a high-flow homopolymer polypropylene nucleated and anti static designed for the high speed molding of thin-walled, multi-cavity parts. ApplicationTypical appl.. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256 |
A. Schulman PP 1248-01 Polypropylene High-Flow Homopolymer Polypropylene DescriptionPolypropylene PP 1248-01 is a high-flow homopolymer polypropylene nucleated and anti static designed for the high speed molding of thin-walled, multi-cavity parts. ApplicationTypical appl.. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3443U UV Resistant Homopolymer Polypropylene DescriptionPolyfort® FPP 3443U is a 40% talc fortified UV resistant homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256 |
A. Schulman PP 3369-01 Polypropylene Medium-Flow Homopolymer Polypropylene DescriptionPolypropylene PP 3369-01 is a medium-flow homopolymer polypropylene nucleated and anti-static designed for the molding of thin walled, and large parts.ApplicationTypical applications of P.. |
|||
Izod Impact, Notched | 0.260 J/cm @Temperature 23.0 °C |
0.487 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Braskem H 201 Fiber Extrusion Polypropylene Applications: Staple fibers for carpets and blankets; continuous filament for ropes, cords and rugs. Information provided by Braskem |
|||
Izod Impact, Notched | 0.260 - 0.590 J/cm @Thickness 6.35 - 6.35 mm |
0.487 - 1.11 ft-lb/in @Thickness 0.250 - 0.250 in |
Average value: 0.330 J/cm Grade Count:2 |
Overview of materials for Acrylic, Impact Modified, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Izod Impact, Notched | 0.260 J/cm - NB | 0.487 ft-lb/in - NB | Average value: 1.41 J/cm Grade Count:631 |
Overview of materials for Polypropylene Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp.. |