Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.278 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
0.520 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Edgetek® CY-20GF/000 UV FR V0 PC/ABS Blend, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedIgnition ResistantNon-HalogenatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Izod Impact, Notched | 0.278 - 3.04 J/cm | 0.520 - 5.70 ft-lb/in | Average value: 1.14 J/cm Grade Count:79 |
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi.. |
|||
Izod Impact, Notched | 0.278 J/cm | 0.521 ft-lb/in | ASTM D256A |
DSM Somos® 7110 Epoxy Photopolymer, UV Postcure
(discontinued **) DescriptionDSM Somos® 7110 Photopolymer is a humidity-tolerant, high heat-deflection-temperature, low-curl, high-speed liquid that produces rigid, highly accurate parts. It produces exceptional, u.. |
|||
Izod Impact, Notched | 0.278 - 0.641 J/cm | 0.520 - 1.20 ft-lb/in | Average value: 0.508 J/cm Grade Count:10 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler". Specific grades with carbon fiber content bet.. |
|||
Izod Impact, Notched | 0.278 J/cm @Temperature 22.8 °C |
0.520 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Teknor Apex Sinpolene TPP1010 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Talc Filler, 10% Filler by Weight Uses: Appliance Components; Housings Forms: Pellets Processing Method: Injection Mol.. |
|||
Izod Impact, Notched | 0.278 J/cm | 0.520 ft-lb/in | |
Tra-Con Tra-Bond 2248 High Temperature Epoxy Staking Adhesive TRA-BOND 2248 is a thixotropic, high temperature cure, 100% solids epoxy resin system that provides strong, tough bonds between a wide range of materials (includes metals, glass, ceramics, and many .. |
|||
Izod Impact, Notched | 0.278 J/cm | 0.520 ft-lb/in | ASTM D256 |
Ensinger Tecapeek® XP-93 Compression Molded PEEK Compound, 30% PTFE Filled Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Izod Impact, Notched | 0.278 J/cm | 0.520 ft-lb/in | ASTM D256 |
Ensinger Tecatron® XP-86 Compression Molded PPS Compound, with 40% Carbon Fiber Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Izod Impact, Notched | 0.278 J/cm | 0.520 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0336G10CL Glass Reinforced Coupled |
|||
Izod Impact, Notched | 0.278 J/cm | 0.520 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0339W30L1 Wollastonite Reinforced |
|||
Izod Impact, Notched | 0.278 J/cm | 0.520 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0339W40L1 Wollastonite Reinforced |
|||
Izod Impact, Notched | 0.278 J/cm | 0.520 ft-lb/in | ASTM D256 |
Amco Amalloy® B9714 Polymer Alloy Amco Amalloy B9714 is a clear performance copolymer with exceptional clarity and toughness.High elongation before breakage, good melt Flow.Information provided by Amco Plastic Materials. |
|||
Izod Impact, Notched | 0.278 J/cm @Temperature 22.8 °C |
0.520 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Teknor Apex Sinpolene CPP1020 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Calcium Carbonate Filler, 20% Filler by Weight Features: Homopolymer Uses: Appliance Components; Furniture; Housings F.. |