Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.350 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.656 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Novablend™ 5035 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 0.350 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.656 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ GB 1200 30 HS BLACK 18 Polyamide 66 (Nylon 66) Preliminary Data SheetMolded Test Bars: Dry as MoldedInformation provided by PolyOne |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256 |
SABIC PP 528K Polypropylene Homopolymer for Thermoforming Product Description: PP 528K is formulated with an advanced nucleating additive and was specially developed for in-line and off-line thermoforming applications. PP528K exhibits the following featu.. |
|||
Izod Impact, Notched | 0.350 - 0.450 J/cm | 0.656 - 0.843 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ DM_4310 Polypropylene-like Prototyping Polymer Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific conc.. |
|||
Izod Impact, Notched | >= 0.350 J/cm @Temperature 23.0 °C |
>= 0.656 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
NIZHNEKAMSKNEFTEKHIM PP 4316M (EP1X35AF) Propylene and Ethylene Copolymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256 |
PolyOne Edgetek® ET6620-0020 FRV0 Polyamide 66 (Nylon 66) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Izod Impact, Notched | 0.350 - 0.800 J/cm | 0.656 - 1.50 ft-lb/in | Average value: 0.575 J/cm Grade Count:15 |
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and .. |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256 |
NCMT NanoPAC™ HG602 High Performance Polypropylene Nanocomposite Applications: Household Industry Electrical AppliancesInformation provided by Nano Composite Materials Technology Limited |
|||
Izod Impact, Notched | 0.350 - 0.350 J/cm @Temperature -40.0 - -20.0 °C |
0.656 - 0.656 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 0.350 J/cm Grade Count:1 |
Overview of materials for Nylon 66, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature 23.0 °C |
0.656 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® HV-1010 General Purpose PBT, Unreinforced, High Viscosity LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem HC 7260 LS-L HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -20.0 °C |
0.656 ft-lb/in @Temperature -4.00 °F |
ASTM D256-03 |
Ipiranga Petrochem PCC 4414 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Izod Impact, Notched | 0.350 - 0.450 J/cm | 0.656 - 0.843 ft-lb/in | ASTM D256 |
Loxim 820 02T V0 Polypropylene Compound, 20% Talc Filled, Flame Retardant Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL V02570 PPE+HIPS (Asia Pacific) Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL V03505 PPE+HIPS Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Asia Pacific) Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RL004 PA 66 LNP* LUBRICOMP* RL004 is a copmpound based on Nylon 66 resin containing 20% PTFE. Added feature of this grade includes: Wear Resistant. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -30.0 °C |
0.656 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics ULTEM 1010K PEI (Asia Pacific) Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -30.0 °C |
0.656 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics ULTEM 9011 PEI (Europe-Africa-Middle East) Transparent, high flow Polyetherimide (Tg 217C). Resin is RoHS compliant. Improved processability for Fiber extrusion. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -30.0 °C |
0.656 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics ULTEM HU1010 PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI),.. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -30.0 °C |
0.656 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® HX3061HP PBT PBT for compounding/fibers only. Not intended for injection molding. Biocompatible. Melt viscosity: 250C at 21.6 kgf is 1450-1850 poise. Available in Natural color (1001) only. |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 815F PBT+PET (Asia Pacific) PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3727 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3727 is a 24% mineral filled copolymer polypropylene compound.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256 |
Plenco 6990 Phenolic, Briquette, Injection Molded PLENCO 06990 is a glass and mineral filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco. |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256 |
Total PPH 3576 BB Polypropylene Homopolymer, Cast Film Polypropylene 3576 BB is recommended for use in non-oriented cast films processes. It contains an optimized level of slip and anti-block additives.3576 BB is intended for food, magazine or textile .. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature 23.0 °C |
0.656 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamSter PF340S6 PBT, 30% Glass Beads 30% Glass beads reinforced PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature 23.0 °C |
0.656 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Braskem H 503 Injection Molding Polypropylene Description: H 503 is a low melt flow rate additivated homopolyme used for general purposes. It is designed for injection molding, raffia extrusion, bioriented film and general extrusion. This produ.. |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM-D256 |
Braskem HC7260LS-L HDPE Injection Molding Polyethylene HC7260LS-L is a high-density polyethylene developed for injection molding. It has high hardness and stiffness and low warpage. This resin also has additives against ultraviolet radiation action. Its.. |
|||
Izod Impact, Notched | 0.350 - 0.450 J/cm @Temperature -40.0 - -40.0 °C |
0.656 - 0.843 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.400 J/cm Grade Count:1 |
Overview of materials for Nylon 66, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu.. |
|||
Izod Impact, Notched | 0.350 - 2.99 J/cm @Temperature -40.0 - -40.0 °C |
0.656 - 5.60 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 1.52 J/cm Grade Count:12 |
Overview of materials for Nylon 6, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri.. |