Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.200 J/cm @Temperature -18.0 °C |
0.375 ft-lb/in @Temperature -0.400 °F |
ASTM D256 |
Plaskolite Duraplex® 30% I Impact Modified Acrylic Sheet Continuously processed acrylic sheet.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Izod Impact, Notched | 0.200 J/cm @Temperature -18.0 °C |
0.375 ft-lb/in @Temperature -0.400 °F |
ASTM D256 |
Plaskolite Optix® Acrylic Sheet Optix® is a continuously processed acrylic sheet that is crystal clear, impact resistant, weather resistant, and non-yellowing. It offers high molecular weight for superior thermoforming, bending,.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ DM_8210 Rigid Opaque Prototyping Polymer Primary material: VeroBlueSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide the .. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | ASTM D256-06 |
Proto3000 Objet VeroBlue FullCure840 Rigid Opaque Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Izod Impact, Notched | 0.200 J/cm @Diameter 3.17 mm |
0.375 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ASTM D256 |
Ineos Nova 2511 General Purpose Crystal Polystyrene
(discontinued **) High speed molding, Improved crack resistance, USP Class VIApplications: Cutlery, Light louvers, RazorsExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the phy.. |
|||
Izod Impact, Notched | 0.200 J/cm @Diameter 3.17 mm |
0.375 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ASTM D256 |
Ineos Nova 2100 General Purpose Crystal Polystyrene
(discontinued **) Relative high heat resistance, Improved crack resistance, Good strengthApplications: Foam extrusion, Biaxially oriented sheet, Thermoforming applications, Molded packagingExposure to gamma radiation.. |
|||
Izod Impact, Notched | 0.200 J/cm | 0.375 ft-lb/in | ASTM D256 |
Ineos Nova 50 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High strength crystal polystyrene, High heat crystal polystyrene, Custom colorsApplications: Injection molding or extrusion, Designed for applications requiring strength and high heat resistance whe.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar |
Ineos H13G-00 Polypropylene Homopolymer
(discontinued **) Formerly Amoco® 7444. Suggested fabrication methods: Injection moldingFeatures: General purposeTypical applications: Rigid packaging, Medical componentsComplies with FDA specification, Title 21, C.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar |
Ineos H00M-01 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Extrusion; ThermoformingFeatures: High melt strength, High stiffness, Medium-term heat agingComplies with FDA specification, Title 21, CFR 177.1520.Typical application.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H03G-03 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: ExtrusionFeatures: Ease of processingTypical applications: Oriented filmComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from inject.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H20Z-01 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Rigid packaging, Consumer productsComplies with FDA specification, Title 21, CFR 177.1520.Typical.. |
|||
Izod Impact, Notched | 0.200 - 3.93 J/cm | 0.375 - 7.36 ft-lb/in | Average value: 1.34 J/cm Grade Count:5 |
Overview of materials for Silicone, Molded, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
Izod Impact, Notched | 0.200 J/cm | 0.375 ft-lb/in | ASTM D256 |
Plenco Valite 4224 Novolac Phenolic, Granular, Transfer Molded
(discontinued **) This Valite product has been replaced by Plenco 4224. Data provided by Plenco.VALITE 4224 is a brown, two stage, general purpose phenolic molding compound. It has good electrical and moldability ch.. |
|||
Izod Impact, Notched | 0.200 J/cm | 0.375 ft-lb/in | 23° C; ASTM D256 |
Flint Hills P4G4Z-011 Homopolymer Polypropylene Homopolymer, UL certified, USP Class VI certified, and FDA compliant.Features: Applications: Injection molding: general purpose, extruded decorative ribbon, and extruded fiber.Former Huntsman polypr.. |
|||
Izod Impact, Notched | 0.200 J/cm | 0.375 ft-lb/in | ASTM D256 |
Flint Hills P9H8M-058X Specialty Polypropylene Features: Does not contain animal derived components. Product is Phthalate-free. A low phosphorus content material.Applications: Extrusion coating. Suitable for silicone coating.Information pro.. |
|||
Izod Impact, Notched | 0.200 J/cm | 0.375 ft-lb/in | ASTM D256 |
Kolon KOCETAL® TC704 Mineral Reinforced Acetal Resin Whisker reinforced, improved wear and dimensional property. Applications: Dimensionally precise products. Information provided by API-Kolon. |
|||
Izod Impact, Notched | 0.200 J/cm @Diameter 3.17 mm |
0.375 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ASTM D256 |
Ineos Nova 1300 High Heat Crystal Polystyrene High heat resistance, High strength, Good processing characteristics, USP Class ViApplications: Electronics packaging, Medical packaging, Cosmetic cases, Profile extrusionExposure to gamma radiation.. |
|||
Izod Impact, Notched | 0.200 J/cm | 0.375 ft-lb/in | ASTM D882 |
Spartech Polycast UF96 Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Izod Impact, Notched | 0.200 J/cm | 0.375 ft-lb/in | ASTM D256 |
SPS Guang Zhou SAMATâ„¢ EP 5001(f1) Flame-retarded Polypropylene Characteristic: Good flame retardance, non-halogen, high flow properties, high rigidity, high heat resistance, meets the requirements of RoHs and PaHs, excellent UV resistanceApplications: X'mas dec.. |
|||
Izod Impact, Notched | 0.200 J/cm | 0.375 ft-lb/in | ASTM D256 |
Styrolution NAS® 90 High Performance Styrenic NAS® 90 has sparkling clarity, improved toughness, and good scratch resistance. This easily processed copolymer blends well with clear impact modifiers. It meets USP XXIII Spec. of Class VI Pla.. |
|||
Izod Impact, Notched | 0.200 J/cm @Thickness 3.20 mm |
0.375 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Supreme Petrochem SC 203 LV General Purpose Polystyrene CharacteristicsGood flow grade with good mechanical properties Good clarity and flexibility Easy processing grade and suitable for thin walled applicationsProcessing Extrusion MoldingApplicationsSu.. |
|||
Izod Impact, Notched | 0.200 J/cm @Thickness 3.20 mm |
0.375 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Supreme Petrochem SC 206 General Purpose Polystyrene CharacteristicsGood flow grade with clarity & shine Improves aesthetics of final product Processing MoldingApplications Crystal ware, paper weights, house ware Beads, Bangles, gift articles, trays,.. |
|||
Izod Impact, Notched | 0.200 J/cm @Temperature -30.0 °C |
0.375 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL EXNL1117 PPE+HIPS high gloss Noryl |
|||
Izod Impact, Notched | 0.200 J/cm @Temperature 23.0 °C |
0.375 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTAPROP H0260 MC/EC Conductive Polypropylene, Mineral Filled Information provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.200 J/cm | 0.375 ft-lb/in | ASTM D256 |
Ineos Nova 817 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High flow crystal polystyrene, Custom colorsApplications: Injection molding, Designed for use in high speed, Thin section applications and complex parts designs where custom coloring is a requiremen.. |
|||
Izod Impact, Notched | 0.200 - 0.534 J/cm | 0.375 - 1.00 ft-lb/in | Average value: 0.276 J/cm Grade Count:7 |
Overview of materials for Polymethylpentene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polymethylpentene, Molded". Each property range of values reported is minimum and maximum values of appr.. |
|||
Izod Impact, Notched | 0.200 - 0.500 J/cm @Temperature -18.0 - -18.0 °C |
0.375 - 0.937 ft-lb/in @Temperature -0.400 - -0.400 °F |
Average value: 0.325 J/cm Grade Count:4 |
Overview of materials for Acrylic, Impact Modified Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified Sheet". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched | 0.200 J/cm @Diameter 3.17 mm |
0.375 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ASTM D256 |
Ineos Nova 1301 High Heat Crystal Polystyrene High heat resistance, High strength, Good processing characteristics, USP Class VIApplications: Electronics packaging, Medical packaging, Cosmetic cases, Profile extrusionExposure to gamma radiation.. |
|||
Izod Impact, Notched | 0.200 J/cm @Diameter 3.17 mm |
0.375 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ISO 180 |
Ineos Nova 205 Crystal Polystyrene General Purpose Grade
(discontinued **) Easy flow, Good mechanical property balance, Extrusion and Injection MoldingApplications: Sheet and film extrusion, Gloss capping, Blending with HIPS or SBSProperties were determined on injection m.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar |
Ineos H13Z-00 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Packaging, Consumer productsComplies with FDA specification, Title 21, CFR 177.1520.Typical prope.. |