Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.380 J/cm @Temperature -30.0 °C |
0.712 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® C7240P PC+ABS (Asia Pacific) Cycoloy* C7240P resin is a mineral filled, flame retardant PC/ABS. High stiffness combined with balanced flow and impact performance, makes it a good condidate for various applications. |
|||
Izod Impact, Notched | 0.380 J/cm @Temperature 23.0 °C |
0.712 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Reliance Industries Repol H080EY Polypropylene REPOL Polypropylene H080EY is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Izod Impact, Notched | 0.380 J/cm @Temperature 23.0 °C |
0.712 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Faradex EX06464 PEI (Asia Pacific) LNP* Faradex* EX06464 is a compound based on Polyetherimide resin containing Stainless Steel. Added features of this material include: Electrically
Conductive, EMI/RFI Shielding.This data was suppli.. |
|||
Izod Impact, Notched | 0.380 J/cm | 0.712 ft-lb/in | ASTM D256 |
Gharda Chemicals Gafone™ 3610GM20 Polyethersulfone (PES)
(discontinued **) Characteristics: Excellent Thermal Resistance - Tg 224°C Outstanding Mechanical, Electrical, Flame & Chemical Resistance Very good Hydrolytic & Sterilization Resistance Good Optical Cl.. |
|||
Izod Impact, Notched | 0.380 J/cm | 0.712 ft-lb/in | ASTM D256 |
Ineos J60-1700-173 HDPE J60-1700-173 is a high density polyethylene homopolymer. This resin is a product of Ineos' technology and is characterized by a narrow molecular weight distribution. Parts fabricated from this mater.. |
|||
Izod Impact, Notched | 0.380 J/cm @Temperature 23.0 °C |
0.712 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
IRPC Polimaxx Polene 3342R Polypropylene Random Copolymer CHARACTERISTICS: HIGH CLARITY, HIGH FLOW, GOOD PROCESSABILITY APPLICATIONS: INJECTION MOLDING FOR FOOD CONTAINERS, HOUSEWARES, CRATES |
|||
Izod Impact, Notched | 0.380 J/cm @Temperature -20.0 °C |
0.712 ft-lb/in @Temperature -4.00 °F |
|
Kuraray HYBRAR® PH4 Polypropylene Blend Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Izod Impact, Notched | >= 0.380 J/cm | >= 0.712 ft-lb/in | Method A; ASTM D 256 |
Karina 805-10/152-A-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Izod Impact, Notched | >= 0.380 J/cm | >= 0.712 ft-lb/in | Method A; ASTM D 256 |
Karina E 830-10/145-A-ERYB-LMP White PVC Compound Heavy metal free PVC compound recommended for extrusion of profiles for general applications. It is supplied in pellet form and should be processed at the temperature range of 170°C to 190°C... |
|||
Izod Impact, Notched | 0.380 J/cm | 0.712 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP ML003S PP LNP* LUBRICOMP* ML003S is a compound based on Polypropylene resin containing 15% PTFE. Added features include: Heat Stabilized, Wear Resistant. |
|||
Izod Impact, Notched | 0.380 J/cm | 0.712 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 325FC PBT (Europe-Africa-Middle East) Commercial, VALOX 325FC is compliant with food contact regulations. VALOX 325FC is a general purpose, unreinforced PBT injection moulding resin which contains internal mold release. This new 325FC g.. |
|||
Izod Impact, Notched | 0.380 J/cm | 0.712 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP WH0200B PBT LNP* Thermocomp* WH0200B is a compound based on PBT resin containing proprietary fillers. Added features include: High Specific Gravity. |
|||
Izod Impact, Notched | 0.380 J/cm @Temperature -30.0 °C |
0.712 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL LTA1350 PPE+PS (Asia Pacific) Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
Izod Impact, Notched | 0.380 J/cm @Temperature -30.0 °C |
0.712 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL LTA5020 PPE+PS Noryl* LTA5020 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
Izod Impact, Notched | 0.380 J/cm @Temperature -30.0 °C |
0.712 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics ULTEM AUT210 PEI (Asia Pacific) Transparent Polyetherimide (Tg 227 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature o.. |
|||
Izod Impact, Notched | 0.380 J/cm @Temperature -30.0 °C |
0.712 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics ULTEM AUT210 PEI (Europe-Africa-Middle East) Transparent Polyetherimide (Tg 227 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature o.. |
|||
Izod Impact, Notched | 0.380 J/cm | 0.712 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP MF002S PP LNP* Thermocomp* MF002S is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched | 0.380 J/cm | 0.712 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Asia Pacific) Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |
|||
Izod Impact, Notched | 0.380 J/cm | 0.712 ft-lb/in | ASTM D256 |
Plenco 1581 Polyester, Pellet, Injection Molded PLENCO 01581 is a glass and mineral reinforced pelletized polyester molding compound, exhibiting excellent dimensional stability, mechanical strength and also arc resistance, track resistance, and f.. |
|||
Izod Impact, Notched | 0.380 J/cm | 0.712 ft-lb/in | ASTM D256 |
Toyobo VYLOPET® EMC317A Injection Molding Polyester Resin, Warpageless Applications: Iron's heat insulation plateChair framesHousingsFeatures: WarpagelessInformation provided by Toyobo. |
|||
Izod Impact, Notched | 0.380 J/cm | 0.712 ft-lb/in | ASTM D256 |
Plenco 6500 Phenolic, Briquette, Transfer Molded PLENCO 06500 is a glass reinforced phenolic molding compound offering improved strength, dimensional stability, and excellent electrical properties. UL recognized under component file E40654. 06500 .. |
|||
Izod Impact, Notched | 0.380 J/cm | 0.712 ft-lb/in | ASTM D256 |
Cresset Powers Cress-Alon™ NE2740 4% Nano Clay Loaded, 2.7 r.v. Compounding Grade Nylon 6, 50% RH Low density, high rigidity, high heat distortion temperature, high retention of mechanical properties under humid conditions, flame retardant, recyclable and environmentally friendly, less glass fib.. |
|||
Izod Impact, Notched | 0.380 - 1.50 J/cm @Temperature -40.0 - -20.0 °C |
0.712 - 2.81 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 0.940 J/cm Grade Count:1 |
Overview of materials for Low Density Polyethylene (LDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum .. |
|||
Izod Impact, Notched | 0.380 J/cm | 0.712 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL FP6130 PPE+PS Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |
|||
Izod Impact, Notched | 0.380 J/cm | 0.712 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL RN0611 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0611 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen.. |
|||
Izod Impact, Notched | 0.380 J/cm | 0.712 ft-lb/in | ASTM D256 |
Sumitomo Bakelite North America Epiall® 1914A Short Glass Fiber Reinforced Epoxy Epiall 1914A is a short fiberglass reinforced epoxy molding compound, with excellent dimensional stability, good strength properties and good electrical insulation properties.Information provided by.. |
|||
Izod Impact, Notched | 0.380 J/cm | 0.712 ft-lb/in | ASTM D256A |
Sumitomo Bakelite North America FM 4017F Fiberglass and Mineral Reinforced Phenolic FM 4017F is a fiberglass and mineral reinforced phenolic molding compound, with excellent dimensional stability and good strength at elevated temperatures. Information supplied by Sumitomo Bak North.. |
|||
Izod Impact, Notched | 0.380 J/cm | 0.712 ft-lb/in | ASTM D256 |
Sumitomo Bakelite North America RX® 647 Fiberglass Reinforced Phenolic RX 643 is a fiberglass reinforced, ammonia-free, phenolic resole compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type GPI-10. RX 647 is a fibe.. |
|||
Izod Impact, Notched | 0.380 J/cm @Temperature 23.0 °C |
0.712 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Braskem H 510 Bioriented Film Polypropylene Applications: Bioriented films for conversion; adhesive tapes; textile and food packing. Information provided by Braskem |
|||
Izod Impact, Notched | 0.380 J/cm @Temperature 23.0 °C |
0.712 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Braskem H 606 Thermoforming Polypropylene Description: H 606 is low melt flow rate homopolymer with general purpose additive package. This resin is designed for extrusion and thermoforming. H 606 presents excellent processability and high o.. |