Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.210 J/cm | 0.393 ft-lb/in | ASTM D256 |
Plaskolite PL-24 Acrylic Resin For injection molding. An unlubricated version of PL-25 extrusion grade pellets. Highest molecular weight, maximum heat resistance.Information supplied by the manufacturer. |
|||
Izod Impact, Notched | 0.210 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
0.393 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Therma-Tech™ NNC-5000 TC Polyamide 66 (Nylon 66) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Izod Impact, Notched | 0.210 J/cm @Temperature -30.0 °C |
0.393 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics GELOY FXW749SK ASA Sparkle VisualFx ASA Resin - Weatherable |
|||
Izod Impact, Notched | 0.210 J/cm @Thickness 3.17 mm |
0.393 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS SAN-80HF High Flow SAN Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 0.210 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.393 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Cellular E2000 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 0.210 J/cm | 0.393 ft-lb/in | ASTM D256 |
Plenco 4224 Phenolic, Granular, Transfer Molded
(discontinued **) Two-stage Phenolic. PLENCO 04224 is a brown, two stage, general purpose phenolic molding compound. It has good electrical and moldability characteristics. It is used in electrical and automotive ap.. |
|||
Izod Impact, Notched | 0.210 J/cm | 0.393 ft-lb/in | ASTM D256 |
Plenco 308 Black (INJ) Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok 308 is a two-stage, mineral and flock-filled phenolic molding compound designed to withstand the hostile environment of high abrasion and high tangential speed of engine pulleys. It is char.. |
|||
Izod Impact, Notched | 0.210 - 0.490 J/cm | 0.393 - 0.919 ft-lb/in | Average value: 0.399 J/cm Grade Count:4 |
Overview of materials for Nylon 66, 10% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ.. |
|||
Izod Impact, Notched | 0.210 J/cm | 0.393 ft-lb/in | ASTM D256 |
Plaslok 309 Black (INJ) Mineral/Fiber Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 309 is a two-stage, mineral and fiber.. |
|||
Izod Impact, Notched | 0.210 J/cm | 0.393 ft-lb/in | ASTM D256 |
Ineos H20A-00 Polypropylene Homopolymer A controlled rheology polypropylene homopolymer produced by Ineos utilizing unique catalyst technology. It is designed for injection molding applications requiring a moderate level of antistatic ag.. |
|||
Izod Impact, Notched | 0.210 J/cm | 0.393 ft-lb/in | ASTM D256/A |
Iran Petrochemical (PCC) 52528 High Density Polyethylene 52528 is a HDPE copolymer injection molding grade for thin walled applications requiring a good balance between high flowability and physical properties.Application: caps, thin walled, injection mol.. |
|||
Izod Impact, Notched | 0.210 J/cm | 0.393 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RL0019 PA 66 LNP LUBRICOMP* RL0019 is a compound based on Nylon 66 resin containing 5% PTFE. Added features of this material include: Flame Retardant, Wear Resistant. |
|||
Izod Impact, Notched | 0.210 J/cm | 0.393 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RL0049S PA 66 LNP LUBRICOMP* RL0049S is a compound based on Nylon 66 resin containing 20% PTFE. Added features of this material include: Flame Retardant, Heat Stabilized, Wear Resistant. |
|||
Izod Impact, Notched | 0.210 J/cm @Temperature 23.0 °C |
0.393 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp RP0049 PA 66 LNP LUBRICOMP* RP0049 is a compound based on Nylon 66 resin containing Flame Retardant, PTFE, Silicone. Added features of this material include: Flame Retardant.This data was supplied by SABIC-IP f.. |
|||
Izod Impact, Notched | 0.210 J/cm @Temperature 23.0 °C |
0.393 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Stat-kon AE0039 ABS LNP STAT-KON* AE0039 is a compound based on Acrylonitrile Butadiene Styrene resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Electrically Conductive.This dat.. |
|||
Izod Impact, Notched | 0.210 J/cm @Temperature 23.0 °C |
0.393 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Stat-kon AE0039 ABS (Asia Pacific) LNP* STAT-KON* AE0039 is a compound based on Acrylonitrile Butadiene Styrene resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Electrically Conductive.This da.. |
|||
Izod Impact, Notched | 0.210 J/cm | 0.393 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP MB006HS PP (Asia Pacific) LNP* Thermocomp* MB006HS is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched | 0.210 J/cm | 0.393 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP MB006S PP LNP THERMOCOMP* MB006S is a compound based on Polypropylene resin containing 30% Glass Bead. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched | 0.210 J/cm | 0.393 ft-lb/in | ASTM D256A |
Sumitomo Bakelite North America 51-01 CAFR-P Mineral Filled Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ.. |
|||
Izod Impact, Notched | 0.210 J/cm | 0.393 ft-lb/in | ASTM Data |
Dow Tyril® 990 SAN TYRIL® 990 SAN copolymer grade provides colorless glass-like clarity and excellent overall optical properties. It provides a profile of very good strength with stiffness, chemical resistance, heat .. |
|||
Izod Impact, Notched | 0.210 J/cm @Temperature -40.0 °C |
0.393 ft-lb/in @Temperature -40.0 °F |
ASTM Test |
BASF Ultramid® 8202CQ PA6 (Conditioned) Ultramid 8202CQ is a low viscosity, PA6 injection molding homopolymer, possessing a modified crystalline structure or increased property performance and faster cycles. It is also available in pigme.. |
|||
Izod Impact, Notched | 0.210 J/cm @Temperature -40.0 °C |
0.393 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Ashley Polymers Ashlene® D930H Nylon 12 A plasticized Nylon 12 offering improved flexibility with superior moisture and chemical resistance. Also UV and heat stabilized, available in natural and precolored. Any color other than natural .. |
|||
Izod Impact, Notched | 0.210 J/cm | 0.393 ft-lb/in | ASTM D256 |
Bapolene® 4082 Polypropylene, Injection Grade Bapolene PP4082 is a high flow, fast cycle injection molding resin. Injection molded parts exhibit good stiffness and chemical resistance. This product meets FDA standards for food contact applica.. |
|||
Izod Impact, Notched | 0.210 J/cm @Temperature -40.0 °C |
0.393 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Ashley Polymers Ashlene® 831 Nylon 6 General purpose extrusion grade for wire jacketing, tubing, rods, slabs and centrifugal casting. ASHLENE 831 meets FDA requirements and is therefore also suitable for film extrusion and co-extrusio.. |
|||
Izod Impact, Notched | 0.210 - 2.67 J/cm | 0.393 - 5.00 ft-lb/in | Average value: 0.768 J/cm Grade Count:93 |
Overview of materials for Nylon 66, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Izod Impact, Notched | 0.210 J/cm | 0.393 ft-lb/in | 63.5*12.7*3.2mm, Cut; ASTM D256 |
SABIC Innovative Plastics SABIC PPCOMPOUND 15T1020 PP SABIC® PPcompound 15T1020. This grade is a general purpose, talc filled, heat stabilized polypropylene resin suitable for injection molded applications. The IMDS ID is 16486973. |
|||
Izod Impact, Notched | 0.210 - 0.64068 J/cm @Diameter 6.35 - 6.35 mm |
0.393 - 1.2003 ft-lb/in @Diameter 0.250 - 0.250 in |
Average value: 0.330 J/cm Grade Count:10 |
Overview of materials for Acrylic, Impact Modified, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Izod Impact, Notched | 0.210 J/cm @Diameter 3.17 mm |
0.393 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
BP Amoco Accpro® 9433 Enhanced Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: High stiffness, Surface hardness, Stain resistance, Antistatic, NucleatedComplies with FDA specification, Title 21, CFR 177.1520.Typical app.. |
|||
Izod Impact, Notched | 0.210 J/cm | 0.393 ft-lb/in | ASTM D256 |
Plaslok 308 Black (INJ) Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 308 is a two-stage, mineral and flock.. |