Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.430 J/cm | 0.806 ft-lb/in | ISO METHOD 180 |
NYCOA 2061 Copolymer Nylon 6/69 monofilament weed eater, fishing lineInformation provided by NYCOA, Inc. |
|||
Izod Impact, Notched | 0.430 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.806 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ MF 1200 A 40 HS Natural Polyamide 66 (Nylon 66) The Nymax® MF 1200 Series of mineral-reinforced nylon 6/6 compounds have been specifically engineered to provide an excellent balance of physical property performance, toughness, chemical resistanc.. |
|||
Izod Impact, Notched | 0.430 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
0.806 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Stat-Tech™ AS-08CF/000 UV FR V0 Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Izod Impact, Notched | 0.430 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.806 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Stat-Tech™ AS-13CF/000 Black Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Izod Impact, Notched | 0.430 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.806 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Stat-Tech™ NN-40CF/000 NH FRV0 Natural Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Izod Impact, Notched | 0.430 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
0.806 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Therma-Tech™ NN-3000 TC Polyamide 66 (Nylon 66) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Izod Impact, Notched | 0.430 J/cm | 0.806 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics EXTEM XH1005 TPI Resin (Europe-Africa-Middle East) Thermoplastic Polyimide Extem* XH1005 Resin. |
|||
Izod Impact, Notched | 0.430 J/cm @Thickness 3.17 mm |
0.806 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS POM-270 27.0 MFI Acetal Copolymer Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 0.430 J/cm @Temperature -30.0 °C |
0.806 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® ML7677 PC (Asia Pacific) Transparent Polycarbonate in limited colors. Excellent processability, super high flow, flame retardant, UL rated V-1 at 2.0mm |
|||
Izod Impact, Notched | 0.430 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.806 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded; ASTM D256A |
PolyOne Geon™ L6105 natural Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 0.430 - 0.600 J/cm @Temperature -40.0 - -20.0 °C |
0.806 - 1.12 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 0.554 J/cm Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15.. |
|||
Izod Impact, Notched | 0.430 J/cm | 0.806 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers KetaSpire® KT-880P Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880P is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire PEEK is produced to the highest industry standards and is.. |
|||
Izod Impact, Notched | 0.430 J/cm @Thickness 6.35 mm |
0.806 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Lubri-Tech™ NL-000/15T Nylon 612 - 15% PTFE Lubricated
(discontinued **) Properties Dry as MoldedData provided by M. A. Hanna. M. A. Hanna and Geon merged to form PolyOne in 2000. |
|||
Izod Impact, Notched | 0.430 - 0.640 J/cm @Thickness 6.35 mm |
0.806 - 1.20 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Lubri-Tech™ NL-15KV/05M Nylon 6/12 - 15% Kevlar Fiber - 5% MoS2
(discontinued **) Data provided by PolyOne. |
|||
Izod Impact, Notched | 0.430 J/cm | 0.806 ft-lb/in | ASTM D256A |
LyondellBasell Astryn BA905-74 Polypropylene Copolymer, Flame Retardant Key Features: medium high melt flow, medium high modulus, flame retardant, low specific gravity, good impact strengthApplications: battery jars, electrical componentsDescription: Astryn BA905-74 med.. |
|||
Izod Impact, Notched | 0.430 J/cm | 0.806 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-848 CF30 is a 30% carbon fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparabl.. |
|||
Izod Impact, Notched | 0.430 J/cm | 0.806 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI) Torlon® 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not .. |
|||
Izod Impact, Notched | 0.430 J/cm @Temperature 23.0 °C |
0.806 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp AF0029 ABS LNP* Thermocomp* AF0029 is an ABS base resin containing Glass Fiber. Characteristics of this grade are Flame Retardancy.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.430 J/cm @Thickness 3.17 mm |
0.806 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Unitika AX-1500W Dry Characteristics: A resin succeeding the advantages of AX1500 resin and containing titanium oxide at high concentration. Improved drastically in light reflection and blocking properties, aimed at dis.. |
|||
Izod Impact, Notched | 0.430 J/cm @Temperature -40.0 °C |
0.806 ft-lb/in @Temperature -40.0 °F |
Method B; Brittle Failure |
Elastomer Engineering Elastamide 100 Elastomer Modified RIM Nylon 6 30% crystallinity. Information supplied by Elastomer Engineering. |
|||
Izod Impact, Notched | 0.430 J/cm | 0.806 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP1666 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1666 is a 10% talc filled homopolymer polypropylene compound. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.430 J/cm @Temperature 23.0 °C |
0.806 ft-lb/in @Temperature 73.4 °F |
DAM; ASTM D256 |
DuPont Performance Polymers Zytel® FR7025V0F NC010 Nylon 66
(Unverified Data**) Zytel® FR7025V0F NC010 is a flame retardant polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuPont Performance.. |
|||
Izod Impact, Notched | 0.430 J/cm @Thickness 3.17 mm |
0.806 ft-lb/in @Thickness 0.125 in |
ASTM Test |
BASF Ultramid® 8231G HS BK-106 14% Glass Filled PA6 (Dry) Ultramid 8231G HS BK-106 is a black pigmented heat stabilized, 14% glass fiber reinforced PA6 injection molding compound.The glass fiber reinforcement enhances performance such as strength, stiffnes.. |
|||
Izod Impact, Notched | 0.430 J/cm | 0.806 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 829 Nylon 6 Basic Nylon 6, low viscosity, unlubricated.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.430 J/cm | 0.806 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 243 SAN, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.430 J/cm | 0.806 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 105 PBT Polyester A general purpose polyester with low shrinkage and good flow.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.430 J/cm | 0.806 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 828L Nylon 6 Medium viscosity general purpose nylon, complies with NSF under Standard 14 for pipe components.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.430 J/cm | 0.806 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 859 Nylon 6, Pellet form Ashlene 859 is offered in small pellet form. It is dried to less than 0.1% moisture eliminating the need for predrying. Ashlene 859 is molded with wall thickness ranging from 1/16" to greater than.. |
|||
Izod Impact, Notched | 0.430 J/cm | 0.806 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 757 Carbon Fiber Reinforced, Flow Enhanced, PPS Alloy Data provided by the manufacturer, ComAlloy International Company.30% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.430 J/cm @Temperature 23.0 °C |
0.806 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp JF002E PES LNP THERMOCOMP* JF002E is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the America.. |