Mechanical Properties Metric English Comments
Izod Impact, Notched 0.230 J/cm
0.431 ft-lb/in
ASTM D256
SABIC PP 520L Polypropylene Homopolymer for Tubular Water Quenched Film
Product Description: PP 520L is specially developed for tubular water quenched blown film applications with a suitable dosage of slip and antiblock additives.Films produced using PP 520L will exhib..
Izod Impact, Notched 0.230 J/cm

@Temperature -30.0 °C
0.431 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Cycolac® INP562 ABS+SAN
SABIC INP562 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet..
Izod Impact, Notched >= 0.230 J/cm

@Temperature 23.0 °C
>= 0.431 ft-lb/in

@Temperature 73.4 °F
ASTM D256
NIZHNEKAMSKNEFTEKHIM PP 1548S (H32GA) Propylene Homopolymer
Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P..
Izod Impact, Notched 0.230 J/cm
0.431 ft-lb/in
ASTM D256
North Wood Plastics Polypropylene with 60% Wood Fiber, Molding Grade
Data provided by North Wood Plastics, Inc.
Izod Impact, Notched 0.230 J/cm

@Thickness 4.00 mm,
Temperature 23.0 °C
0.431 ft-lb/in

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Premix Thermoplastics PRE-ELEC® ESD 1100  (discontinued **)
PRE-ELEC ESD 1100 is a static dissipative thermoplastic compound based on PETG. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 1100 has been developed for the e..
Izod Impact, Notched 0.230 J/cm
0.431 ft-lb/in
ASTM D256
SABIC Innovative Plastics Cycolac® INP581 ABS+SAN
High flow, low molecular weight SAN. Can be used as compounding additives for polymer blends. Can be blended with high rubber graft modifier resins to produce customized ABS properties. Suitable for..
Izod Impact, Notched 0.230 - 0.570 J/cm

@Temperature -40.0 - -30.0 °C
0.431 - 1.07 ft-lb/in

@Temperature -40.0 - -22.0 °F
Average value: 0.377 J/cm Grade Count:22
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m..
Izod Impact, Notched 0.230 J/cm
0.431 ft-lb/in
ASTM D256
Plenco 7300 Phenolic, Nodular, Transfer Molded  (discontinued **)
Two-Stage Phenolic. PLENCO 07300 is an organic fiber reinforced phenolic molding compound offering improved mechanical strength and excellent cosmetic properties. UL recognized under component file..
Izod Impact, Notched 0.230 J/cm
0.431 ft-lb/in
ASTM D256
Ineos T50-3600 HDPE
Ineos T50-3600 is a high density polyethylene copolymer of narrow molecular weight distribution used primarily for high speed injection molding of thin-walled articles. It is characterized by a hig..
Izod Impact, Notched 0.230 J/cm

@Temperature -40.0 °C
0.431 ft-lb/in

@Temperature -40.0 °F
ISO 180
LyondellBasell Hifaxâ„¢ BB222GC Thermoplastic Olefin Resin
Key Features: medium melt flow, very high modulus, UV-stabilized thermoplastic elastomeric olefin resin, excellent impact and stiffness balance, excellent weatherability, high stiffness, good dimens..
Izod Impact, Notched 0.230 J/cm
0.431 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP STAT-KON DD0001 PC
LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant.
Izod Impact, Notched 0.230 J/cm
0.431 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP STAT-KON DD0001 PC (Asia Pacific)
LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive.
Izod Impact, Notched 0.230 J/cm
0.431 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP STAT-KON DD0001 PC (Europe-Africa-Middle East)
LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive.
Izod Impact, Notched 0.230 J/cm
0.431 ft-lb/in
ASTM D256
Styrolution Styrolux® 684 D SBC
Description: Styrolux® 684 D is a clear styrene-butadiene copolymer (SBC) used in injection molding for parts with enhanced toughness as well as in sheet and film extrusion and blow molding. Part..
Izod Impact, Notched 0.230 J/cm
0.431 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL ZM3242 PPE+PS (Asia Pacific)
Modified PPO* 30% mineral filled products, Non Halogenated Flame Retardant V-1 products.Supper low warpage series, HDT 110degC
Izod Impact, Notched 0.230 J/cm

@Temperature 23.0 °C
0.431 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Thermocomp ZM3242 PPE+PS (Asia Pacific)
Modified PPO* 30% mineral filled products, Non Halogenated Flame Retardant V-1 products.Supper low warpage series, HDT 110degCThis data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched 0.230 J/cm
0.431 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOTUF CF007IXP PS
LNP* Thermotuf* CF007IXP is a compound based on Polystyrene containing glass fiber. Characteristics of this grade are: High Impact.
Izod Impact, Notched 0.230 J/cm
0.431 ft-lb/in
Cosmic Plastics K43 Mineral Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Izod Impact, Notched 0.230 J/cm
0.431 ft-lb/in
Cosmic Plastics D45 Mineral Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Izod Impact, Notched 0.230 - 0.290 J/cm
0.431 - 0.543 ft-lb/in
ASTM D256A
DSM Somos® GP Plus 14122
Somos® GP Plus 14122 is a low-viscosity stereolithography resin with an opaque white appearance. This material mirrors production plastics like ABS and PBT, making it an ideal choice for virtually ..
Izod Impact, Notched 0.230 - 0.510 J/cm
0.431 - 0.955 ft-lb/in
ASTM D256
3D Systems Accura® ClearVue™ Free (SL 7870) Stereolithography Plastic
High clarity plastic for a multitude of applicationsFeaturesClear and transparentRigid and toughGreat for headlamps, bottles and transparent assembliesExcellent humidity/moisture resistanceAll infor..
Izod Impact, Notched 0.230 J/cm
0.431 ft-lb/in
ASTM-D256
Braskem H 125 HOMO Polypropylene Homopolymer
H 125 is a high melt flow rate homopolymer designed for nonwoven by spunbonded processing. It is used in fiber extrusion processing. This resin features excellent processing, allowing increased line..
Izod Impact, Notched 0.230 J/cm
0.431 ft-lb/in
ASTM-D256
Braskem H 214 HOMO Polypropylene Homopolymer
H 214 is a high melt flow rate homopolymer with narrow molecular weight distribution. It is specially designed for fiber extrusion and nonwoven applications. This product presents excellent processa..
Izod Impact, Notched 0.230 J/cm

@Temperature >=23.0 °C
0.431 ft-lb/in

@Temperature >=73.4 °F
ASTM D256
Carmel Olefins CAPILENE® T 50 Polypropylene Homopolymer
CAPILENE® T 50 is a high melt flow rate homopolymer for injection molding characterized by good flow properties combined with good stiffness. APPLICATIONS CAPILENE ® T 50 is recommended for in..
Izod Impact, Notched 0.230 J/cm

@Temperature >=23.0 °C
0.431 ft-lb/in

@Temperature >=73.4 °F
ASTM D256
Carmel Olefins CARMELCOAT™ MT 34 EC Specialty Polypropylene for Extrusion Coating
CARMELCOAT™ MT 34 EC is a specialty polypropylene developed for extrusion coating and lamination. This grade exhibits improved process ability for applications which requires high coating speeds, l..
Izod Impact, Notched 0.230 J/cm

@Thickness 3.20 mm
0.431 ft-lb/in

@Thickness 0.126 in
ASTM D256
Beijing Chemical Industry KAIFA® GL6000 ABS Metal Plating Grade
Excellent plating performance, Good thermal stabilityInformation provided by Beijing Chemical Industry Research Institute (Group)
Izod Impact, Notched 0.230 J/cm
0.431 ft-lb/in
ASTM D256
Plenco 6527 Phenolic, Granular, Injection Molded
PLENCO 06527 is a woodflour and mineral filled resole phenolic molding compound.Information supplied by Plenco.
Izod Impact, Notched 0.230 - 5.82 J/cm
0.431 - 10.9 ft-lb/in
Average value: 2.65 J/cm Grade Count:20
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum..
Izod Impact, Notched 0.230 J/cm
0.431 ft-lb/in
ASTM D256
Plenco 6554 Phenolic, Granular, Compression Molded  (discontinued **)
Two-Stage Phenolic. PLENCO 06554 is an organic reinforced phenolic molding compound modified with PTFE to offer improved coefficient of friction values. 06554 is available in black.Information supp..
Izod Impact, Notched 0.230 J/cm
0.431 ft-lb/in
Cosmic Plastics D44 Mineral Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Copyright © lookpolymers.com All Rights Reserved