Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.247 J/cm | 0.463 ft-lb/in | ASTM D256 |
Plenco 7202 Phenolic, Granular, Injection Molded PLENCO 07202 is an organic fiber reinforced phenolic molding compound, formulated to offer improved mechanical strength properties with an industrial finish. UL recognized under component file E4065.. |