Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.500 J/cm | 0.937 ft-lb/in | ASTM D256 |
Nylene® 609 Nylon 6, Film/Extrusion Grade Dry as molded. Film grade. Nylene 609 is a high viscosity, extrusion resin recommended for practically all types of extrusion including profile, film, and extrusion coating. It is especially recom.. |
|||
Izod Impact, Notched | 0.500 J/cm | 0.937 ft-lb/in | ASTM D256 |
Nylene® PA6/6 Mineral Filled 6140 HS Nylon 6/6 40% Mineral Filler; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature -30.0 °C |
0.937 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® BM5225X PC (Asia Pacific) BM5225X resin is a mineral filled grade featuring of high modulus, good flow and ductility, low warpage. It is of non-Br & non-Cl flame retardant systems intended to meet thin wall flame resistance .. |
|||
Izod Impact, Notched | 0.500 - 0.600 J/cm | 0.937 - 1.12 ft-lb/in | Average value: 0.567 J/cm Grade Count:3 |
Overview of materials for Polyphthalamide (PPA), Stainless Fiber, EMI This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum va.. |
|||
Izod Impact, Notched | 0.500 - 9.77 J/cm | 0.937 - 18.3 ft-lb/in | Average value: 7.04 J/cm Grade Count:82 |
Overview of materials for Polycarbonate, UV Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a.. |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature -40.0 °C |
0.937 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
BASF Capron® 8202 NL Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Izod Impact, Notched | 0.500 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
0.937 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUCEL FW715CS Modified POM, Friction Resistance, Abrasion Resistance Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0 and 471-34-1Information provided by LG .. |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature 23.0 °C |
0.937 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL HG-3250 High Gloss Polypropylene, 25% Mineral Fillers LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature -29.0 °C |
0.937 ft-lb/in @Temperature -20.2 °F |
ASTM D256 |
Global POM-90 General Purpose Acetal Information provided by Global Polymers Corporation. |
|||
Izod Impact, Notched | 0.500 - 0.600 J/cm | 0.937 - 1.12 ft-lb/in | ASTM D256 |
Loxim 830 12 HB Polypropylene Compound, Flame Retardant Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature 23.0 °C |
0.937 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® GP-2151F General Purpose PBT, 15% Glass Fiber Reinforced, Flame Retardant LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature -30.0 °C |
0.937 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS (Asia Pacific) Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature 23.0 °C |
0.937 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp KFL36XXC Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KFL36 is an Acetal containing Glass Fiber and PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 0.500 J/cm | 0.937 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 325 PBT (Europe-Africa-Middle East) VALOX 325 is a general purpose, unreinforced PBT injection moulding resin. Applications: sprinklers and nozzles, pumps, doorhandles, tank covers, pens and pencils. |
|||
Izod Impact, Notched | 0.500 J/cm | 0.937 ft-lb/in | ASTM D256 |
SPS Guang Zhou POPTREEâ„¢ 6001A Flame-retarded Polyethylene Characteristic: Low density, medium melt flow index, medium notched impact strength, no bloomingApplications: E/E partsInformation Provided by SPS (Guang Zhou) Ltd. |
|||
Izod Impact, Notched | 0.500 J/cm | 0.937 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® SHF4930 PBT (Europe-Africa-Middle East) Super high flow FR PBT grade with 15% Glass reinforced |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature -30.0 °C |
0.937 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX674PC PPE+PA6 (Europe-Africa-Middle East) A conductive PPE/PA blend designed to have improved surface appearance and elevated heat resistance for powder coating. The material is suitable for injection molding. The material is only availab.. |
|||
Izod Impact, Notched | 0.500 J/cm | 0.937 ft-lb/in | ISO 180 |
Wellman Wellamid® 22LH-N Unfilled Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae.. |
|||
Izod Impact, Notched | 0.500 J/cm | 0.937 ft-lb/in | ISO 180 |
Wellman Wellamid® MR340 42H-N 34% Mineral Reinforced Nylon 6, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Izod Impact, Notched | 0.500 J/cm @Temperature 23.0 °C |
0.937 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamSter RF350M3 PBT, 15% Mineral Filled 15% mineral filled PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.500 J/cm | 0.937 ft-lb/in | |
Zeon Chemicals Zeonex® RS420 Cyclo-Olefin Polymer |
|||
Izod Impact, Notched | 0.500 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.937 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epinyl PA 6 Polyamide 6 Characteristics: medium viscosity, good mechanical properties |
|||
Izod Impact, Notched | 0.500 J/cm @Thickness 3.20 mm |
0.937 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Beijing Chemical Industry KAIFA® 101 PBT Resin Unreinforced, good toughnessInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Izod Impact, Notched | 0.500 J/cm | 0.937 ft-lb/in | ASTM D256 |
Carmel Olefins CAPILENE® QU 73 AV Propylene Random Copolymer Description: CAPILENE® QU 73 AV is a high melt flow rate, controlled rheology polypropylene random copolymer for injection molding of clear articles. CAPILENE® QU 73 AV is clarified with antista.. |
|||
Izod Impact, Notched | 0.500 J/cm | 0.937 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ixef® 2530/X9027 Polyarylamide, 55% Mineral + Glass Fiber, at Equilibrium (65% RH)
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Izod Impact, Notched | >= 0.500 J/cm @Temperature 23.0 °C |
>= 0.937 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek RA320G6 Nylon 6.6, 30% Glass Fiber, Flame Retardant 30% glass fiber reinforced, flame retardant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.500 J/cm | 0.937 ft-lb/in | ASTM D256 |
Ineos J50-1000-178 HDPE A high density polyethylene copolymer intended for the injection molding of closures for beverages. Because of its high purity and excellent organoleptic properties, this grade is certified as low .. |
|||
Izod Impact, Notched | 0.500 J/cm | 0.937 ft-lb/in | ASTM D256 |
Ineos J50-1000-181 HDPE A high density polyethylene copolymer. It has a narrow molecular weight distribution and is intended for the injection molding of screw caps dedicated to the packaging of still water. This resin c.. |
|||
Izod Impact, Notched | 0.500 J/cm | 0.937 ft-lb/in | ASTM D256 |
Ineos J50-1000-187 HDPE A high density polyethylene copolymer. It has a narrow molecular weight distribution and is intended for the injection molding of screw caps dedicated to the packaging of still water. This resin con.. |
|||
Izod Impact, Notched | 0.500 - 3.00 J/cm @Temperature -20.0 - 0.000 °C |
0.937 - 5.62 ft-lb/in @Temperature -4.00 - 32.0 °F |
Average value: 1.14 J/cm Grade Count:4 |
Overview of materials for Polypropylene, Sheet/Thermoforming Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Sheet/Thermoforming Grade". Each property range of values reported is minimum and maximum.. |