Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.270 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.506 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Maxxam™ DP-9162-3 Polypropylene, Unspecified (PP, Unspecified) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Izod Impact, Notched | 0.270 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.506 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Maxxam™ PD 20 TF Black Polypropylene, Unspecified (PP, Unspecified) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Izod Impact, Notched | 0.270 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.506 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Maxxam™ PD 40 TF Black Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Izod Impact, Notched | 0.270 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.506 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Maxxam™ PPH-40T Nat Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Izod Impact, Notched | 0.270 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
0.506 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Therma-Tech™ LC-6000 TC Liquid Crystal Polymer (LCP) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Izod Impact, Notched | 0.270 J/cm @Temperature -40.0 °C |
0.506 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Rotuba 860MH 686.4 Ethyl Cellulose Data provided by the manufacturer. |
|||
Izod Impact, Notched | 0.270 - 0.520 J/cm @Temperature -40.0 - -40.0 °C |
0.506 - 0.974 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.360 J/cm Grade Count:3 |
Overview of materials for PETG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Izod Impact, Notched | 0.270 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.506 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® ET5200-0018 UV RS Desert Sage Polypropylene Homopolymer (PP Homopolymer) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | ASTM D256 |
Plenco 307 Black Impact Grade Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok 307 is a two-stage, mineral and flock-filled phenolic molding compound designed for the automotive industry for use in brake system components. It is characterized by good molding latitude .. |
|||
Izod Impact, Notched | 0.270 - 1.33 J/cm | 0.506 - 2.50 ft-lb/in | Average value: 0.776 J/cm Grade Count:80 |
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma.. |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | ASTM D256A |
LyondellBasell Astryn BA66K Polypropylene Copolymer, Flame Retardant Key Features: high melt flow, medium modulus, flame retardant polypropylene copolymer, high limiting oxygen index, non-halogenated, good aesthetics, excellent processabilityApplications: batteries, .. |
|||
Izod Impact, Notched | 0.270 J/cm @Temperature -40.0 °C |
0.506 ft-lb/in @Temperature -40.0 °F |
ASTM Test |
Styrolution Luran® S 757 G ASA Luran S 757 G is an easy flowing injection molding ASA grade with large flow path/wall thickness ratios.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Izod Impact, Notched | 0.270 J/cm @Thickness 3.17 mm |
0.506 ft-lb/in @Thickness 0.125 in |
ASTM Test |
Styrolution Styrolux 3G33 SBC Styrolux 3G33 is a thermoplastic styrene-butadiene block copolymer which is suitable for injection molding, extrusion and thermoforming. It offers an outstanding combination of crystal clarity and .. |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | ASTM D256 |
A. Schulman PP 1449-01 Polypropylene General-Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1449-01 Natural is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness.ApplicationPP 1449-01 m.. |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1007X Extra High Flow, Talc Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1007X is an extra high flow, 40% talc fortified homopolymer polypropylene. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 809 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 809 is a 40% talc-filled homopolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | ASTM D256 |
A. Schulman PP 1449-01 Polypropylene General-Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1449-01 Natural is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness.ApplicationPP 1449-01 m.. |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RPP 1174 Talc Filled, Homopolymer Polypropylene DescriptionPolyflam® RPP 1174 is a high performance talc filled homopolymer polypropylene product with UL V0 flammability and 105°C temperature index at 0.81 mm. RPP 1174 is non-dripping and has .. |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | |
Cosmic Plastics E4920 Mineral Filled Epoxy Molding Compound, Encapsulated Grade Data provided by the manufacturer. |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | ASTM D256, Notch |
Cresset Powers Cress-Alon™ NF3020 2% Nano Clay Loaded, 3.0 r.v. Film Grade Nylon 6, Dry As Molded Low density, high rigidity, high heat distortion temperature, high retention of mechanical properties under humid conditions, flame retardant, recyclable and environmentally friendly, less glass fib.. |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | ASTM D256, Notch |
Cresset Powers Cress-Alon™ NF3040 4% Nano Clay Loaded, 3.0 r.v. Film Grade Nylon 6, Dry As Molded Low density, high rigidity, high heat distortion temperature, high retention of mechanical properties under humid conditions, flame retardant, recyclable and environmentally friendly, less glass fib.. |
|||
Izod Impact, Notched | 0.270 J/cm @Thickness 3.17 mm |
0.506 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Entec Hypro™ PP-HP20 Homopolymer, 20 Melt Flow This product can be used for general purpose injection molding as well as fiber spinning and other critical extrusion applicationsInformation provided by Entec |
|||
Izod Impact, Notched | 0.270 J/cm @Temperature 23.0 °C |
0.506 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Braskem H 306 Fiber Extrusion Polypropylene Applications: Staple fibers for carpets and blankets. Information provided by Braskem |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | ASTM D-785 |
Bapolene® 4017 Polypropylene Bapolene 4017 is a homopolymer polypropylene with outstanding modulus. It complies with FDA 21 CFR1777.1520.Applications: Strapping, profile extrusion, and general purpose.Bapolene® and Bapolan® .. |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | ASTM D256 |
Bapolene® 4052F Polypropylene, Blown Film Grade Bapolene PP4052F is a PP homopolymer for blown film applications. It contains slip and antiblock additives as processing aids. It offers good clarity and optical properties. This product meets FD.. |
|||
Izod Impact, Notched | 0.270 - 1.07 J/cm | 0.506 - 2.00 ft-lb/in | Average value: 0.534 J/cm Grade Count:27 |
Overview of materials for Acetal Homopolymer, PTFE-Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 627 Nylon 6/6, Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.20% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RPP 1174 Talc Filled, Homopolymer Polypropylene DescriptionPolyflam® RPP 1174 is a high performance talc filled homopolymer polypropylene product with UL V0 flammability and 105°C temperature index at 0.81 mm. RPP 1174 is non-dripping and has .. |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1007X Extra High Flow, Talc Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1007X is an extra high flow, 40% talc fortified homopolymer polypropylene. Information provided by A. Schulman. |